Quantum Efficiency Loss after PID Stress: Wavelength Dependence on Cell Surface and Cell Edge

It is known that the potential induced degradation (PID) stress of conventional p-base solar cells affects power, shunt resistance, junction recombination, and quantum efficiency (QE). One of the primary solutions to address the PID issue is a modification of chemical and physical properties of antireflection coating (ARC) on the cell surface. Depending on the edge isolation method used during cell processing, the ARC layer near the edges may be uniformly or non-uniformly damaged. Therefore, the pathway for sodium migration from glass to the cell junction could be either through all of the ARC surface if surface and edge ARC have low quality or through the cell edge if surface ARC has high quality but edge ARC is defective due to certain edge isolation process. In this study, two PID susceptible cells from two different manufacturers have been investigated. The QE measurements of these cells before and after PID stress were performed at both surface and edge. We observed the wavelength dependent QE loss only in the first manufacturer's cell but not in the second manufacturer's cell. The first manufacturer's cell appeared to have low quality ARC whereas the second manufacturer's cell appeared to have high quality ARC with defective edge. To rapidly screen a large number of cells for PID stress testing, a new but simple test setup that does not require laminated cell coupon has been developed and is used in this investigation.

14 SOLAR ENERGY↗

Effects of Photovoltaic Module Soiling on Glass Surface Resistance and Potential-Induced Degradation

The sheet resistance of three soil types (Arizona road dust, soot, and sea salt) on glass were measured by the transmission line method as a function of relative humidity (RH) between 39% and 95% at 60 degrees C. Sea salt yielded a 3.5 orders of magnitude decrease in resistance on the glass surface when the RH was increased over this RH range. Arizona road dust showed reduced sheet resistance at lower RH, but with less humidity sensitivity over the range tested. The soot sample did not show significant resistivity change compared to the unsoiled control. Photovoltaic modules with sea salt on their faces were step-stressed between 25% and 95% RH at 60 degrees C applying -1000 V bias to the active cell circuit. Leakage current from the cell circuit to ground ranged between two and ten times higher than that of the unsoiled controls. Degradation rate of modules with salt on the surface increased with increasing RH and time.

14 SOLAR ENERGY↗

Quantifying Solar Cell Cracks in Photovoltaic Modules by Electroluminescence Imaging

This article proposes a method for quantifying the percentage of partially and totally disconnected solar cell cracks by analyzing electroluminescence images of the photovoltaic module taken under high- and low-current forward bias. The method is based on the analysis of the module's electroluminescence intensity distribution, applied at module and cell level. These concepts are demonstrated on a crystalline silicon photovoltaic module that was subjected to several rounds of mechanical loading and humidity-freeze cycling, causing increasing levels of solar cell cracks. The proposed method can be used as a diagnostic tool to rate cell damage or quality of modules after transportation. Moreover, the method can be automated and used in quality control for module manufacturers, installers, or as a diagnostic tool by plant operators and diagnostic service providers.

14 SOLAR ENERGY↗

Effects of PV Module Soiling on Glass Surface Resistance and Potential-Induced Degradation

The goals of the project were: Determine applicability of transmission line method (TLM) to evaluate sheet resistance of soils on module glass; Evaluate various soils on glass for changes in surface resistance and their ability to promote potential-induced degradation with humidity (PID); Evaluate PID characteristics, rate, and leakage current increases on full-size mc-Si modules associated with a conductive soil on the surface.

14 SOLAR ENERGY↗

Photovoltaic Module Qualification Plus Testing

This report summarizes a set of test methods that are in the midst of being incorporated into IEC 61215 for certification of a module design or other tests that go beyond certification to establish bankability.

14 SOLAR ENERGY↗

In-Situ Measurement of Crystalline Silicon Modules Undergoing Potential-Induced Degradation in Damp Heat Stress Testing for Estimation of Low-Light Power Performance

The extent of potential-induced degradation of crystalline silicon modules in an environmental chamber is estimated using in-situ dark I-V measurements and applying superposition analysis. The dark I-V curves are shown to correctly give the module power performance at 200, 600 and 1,000 W/m 2 irradiance conditions, as verified with a solar simulator. The onset of degradation measured in low light in relation to that under one sun irradiance can be clearly seen in the module design examined; the time to 5% relative degradation measured in low light (200 W/m 2 ) was 28% less than that of full sun (1,000 W/m 2 irradiance). The power of modules undergoing potential-induced degradation can therefore be characterized in the chamber, facilitating statistical analyses and lifetime forecasting.

14 SOLAR ENERGY↗

Influence of Impurities in Module Packaging on Potential-Induced Degradation

Chemical compounds were added into crystalline silicon cell mini modules, including in the encapsulant, interfaces, and glass, to determine their effect on potential-induced degradation (PID). Fe, either in the glass or at the glass/encapsulant interface, was found to be correlated with increased PID, but the difference in module power loss was not statistically significant compared to controls. Additions of Cu, Cr, Pb, Sn, Ag, and Na compounds to either the encapsulant or at the glass/encapsulant interface did not appear correlated with PID. Lock-in thermography on bare cells affected by PID removed from the mini modules show highly localized areas of junction breakdown, and SIMS analysis indicates localized impurities as well, though a spatial relation between the two was not established. Deposition of a conductive layer on the front surface of the cell, either with semitransparent Ta or Poly 3,4-ethylenedioxythiophene (PEDOT), eliminated PID when the cells were stressed at -1000 V bias, 50°C, with the glass face grounded for 140 h.

14 SOLAR ENERGY↗

Testing and Analysis for Lifetime Prediction of Crystalline Silicon PV Modules Undergoing Degradation by System Voltage Stress: Preprint

Acceleration factors are calculated for crystalline silicon PV modules under system voltage stress by comparing the module power during degradation outdoors to that in accelerated testing at three temperatures and 85% relative humidity. A lognormal analysis is applied to the accelerated lifetime test data considering failure at 80% of the initial module power. Activation energy of 0.73 eV for therate of failure is determined, and the probability of module failure at an arbitrary temperature is predicted. To obtain statistical data for multiple modules over the course of degradation in-situ of the test chamber, dark I-V measurements are obtained and transformed using superposition, which is found well suited for rapid and quantitative evaluation of potential-induced degradation. It isdetermined that shunt resistance measurements alone do not represent the extent of power degradation. This is explained with a two-diode model analysis that shows an increasing second diode recombination current and ideality factor as the degradation in module power progresses. Failure modes of the modules stressed outdoors are examined and compared to those stressed in accelerated tests.

14 SOLAR ENERGY↗

Value Proposition for High Lifetime (p-type) and Thin Silicon Materials in Solar PV Applications: Preprint

Most silicon PV road maps forecast a continued reduction in wafer thickness, despite rapid declines in the primary incentive for doing so -- polysilicon feedstock price. Another common feature of most silicon-technology forecasts is the quest for ever-higher device performance at the lowest possible costs. The authors present data from device-performance and manufacturing- and system-installationcost models to quantitatively establish the incentives for manufacturers to pursue advanced (thin) wafer and (high efficiency) cell technologies, in an age of reduced feedstock prices. This analysis exhaustively considers the value proposition for high lifetime (p-type) silicon materials across the entire c-Si PV supply chain.

14 SOLAR ENERGY↗

NREL Test-to-Failure Protocol (Presentation)

The presentation describes the test-to-failure protocol that was developed and piloted at NREL, stressing PV modules with multiple applications of damp heat (with bias) and thermal cycling until they fail.

14 SOLAR ENERGY↗

Considerations for a Standardized Test for Potential-Induced Degradation of Crystalline Silicon PV Modules (Presentation)

Over the past decade, there have been observations of module degradation and power loss because of the stress that system voltage bias exerts. This results in part from qualification tests and standards note adequately evaluating for the durability of modules to the long-term effects of high voltage bias that they experience in fielded arrays. This talk deals with factors for consideration,progress, and information still needed for a standardized test for degradation due to system voltage stress.

14 SOLAR ENERGY↗

Challenge to Move from 'One Size Fits All' to PV Modules the Customer Needs: Preprint

Historically, PV companies requested a single qualification test for a single product. As the market has grown, there have been increasing opportunities for companies to differentiate their products while still maintaining high manufacturing volumes of each product. At the same time, as PV is deployed in an increasingly broad range of conditions, modules need to be able to withstand a wide rangeof stresses. In some cases, targeting a specific deployment condition may allow reduction of product cost. Realizing this opportunity will require the ability to confidently predict long-term performance based on accelerated tests and known weather conditions. By working together, the community can most quickly develop tests that identify which products perform well under which conditions. Thispaper discusses some of the challenges of predicting long-term PV performance, including the wide range of stresses that may be encountered, the variability of the stresses from moment to moment, the complexity of some degradation mechanisms, and the dependence of accelerated testing on module geometry. The paper also describes two international projects that deal with location-specificdurability evaluation and long-term module performance.

14 SOLAR ENERGY↗

System Voltage Potential-Induced Degradation Mechanisms in PV Modules and Methods for Test: Preprint

Over the past decade, degradation and power loss have been observed in PV modules resulting from the stress exerted by system voltage bias. This is due in part to qualification tests and standards that do not adequately evaluate for the durability of modules to the long-term effects of high voltage bias experienced in fielded arrays. High voltage can lead to module degradation by multiplemechanisms. The extent of the voltage bias degradation is linked to the leakage current or coulombs passed from the silicon active layer through the encapsulant and glass to the grounded module frame, which can be experimentally determined; however, competing processes make the effect non-linear and history-dependent. Appropriate testing methods and stress levels are described that demonstratemodule durability to system voltage potential-induced degradation (PID) mechanisms. This information, along with outdoor testing that is in progress, is used to estimate the acceleration factors needed to evaluate the durability of modules to system voltage stress. Na-rich precipitates are observed on the cell surface after stressing the module to induce PID in damp heat with negative biasapplied to the active layer.

14 SOLAR ENERGY↗

Ensuring Quality of PV Modules: Preprint

Photovoltaic (PV) customers need to have confidence in the PV modules they purchase. Currently, no test can quantify a module's lifetime with confidence, but stress tests are routinely used to differentiate PV product designs. We suggest that the industry would be strengthened by using the wisdom of the community to develop a single set of tests that will help customers quantify confidence in PVproducts. This paper evaluates the need for quality assurance (QA) standards and suggests a path for creating these. Two types of standards are needed: 1) QA of the module design and 2) QA of the manufacturing process.

14 SOLAR ENERGY↗

Exploring diagnostic capabilities for application to new photovoltaic technologies.

Explosive growth in photovoltaic markets has fueled new creative approaches that promise to cut costs and improve reliability of system components. However, market demands require rapid development of these new and innovative technologies in order to compete with more established products and capture market share. Often times diagnostics that assist in R&D do not exist or have not been applied due to the innovative nature of the proposed products. Some diagnostics such as IR imaging, electroluminescence, light IV, dark IV, x-rays, and ultrasound have been employed in the past and continue to serve in development of new products, however, innovative products with new materials, unique geometries, and previously unused manufacturing processes require additional or improved test capabilities. This fast-track product development cycle requires diagnostic capabilities to provide the information that confirms the integrity of manufacturing techniques and provides the feedback that can spawn confidence in process control, reliability and performance. This paper explores the use of digital radiography and computed tomography (CT) with other diagnostics to support photovoltaic R&D and manufacturing applications.

99 GENERAL AND MISCELLANEOUS↗