Engineering Papers⌕ Search

Engineering topics

Hacke, Peter

Publications and source records attributed to Hacke, Peter.

At least 91 records · Page 5

Transmission Electron Microscopy Study on Microstructure of Degraded CdTe Mini-Modules

In this paper, we employ transmission electron microscopy coupled with energy-dispersive X-ray spectrometry (EDS) to study the structure and chemistry of cadmium telluride (CdTe) thin-film solar cells with different extents of degradation. The studied regions originate from the same photovoltaic mini-module, which was subjected to one-sun light exposure at a temperature of 100 degrees C for 400 h to induce light and heat degradation. EDS maps reveal a discontinuous CdS layer and particles rich in O and S but Te-depleted within the CdTe absorber layer after the light and heat stress. These features could act as enhanced recombination centers, resulting in decreased photovoltaic conversion efficiency. Additionally, the most degraded CdTe sample shows a strong accumulation of Na precisely localized in the discontinuous part of the CdS layer. The local Na concentration is determined to be ~16 at.%. In addition, appreciable Na accumulation is observed at the soda-lime glass/transparent conductive oxide interface in both degraded CdTe solar cells. The microstructure of the baseline CdTe mini-module with no stress was also investigated to demonstrate that the structure difference was caused by the light- and heat-induced degradation, instead of module fabrication. These results highlight the need to control the distribution of Na in fielded CdTe modules to sustain long-term high-power output.

14 SOLAR ENERGY↗

Investigating PID Shunting in Polycrystalline CIGS Devices via Multi-Scale, Multi-Technique Characterization

We investigated potential-induced degradation (PID) in CuIn 1-x Ga x Se 2 (CIGS) mini-modules stressed in the laboratory. Small cores were removed from the modules and were subjected to analysis. We completed a proof-of-concept correlative study relating cathodoluminescence to sodium content via time-of-flight secondary-ion mass spectrometry imaging. By comparing one-dimensional depth profile results and three-dimensional tomography results on stressed and unstressed CIGS mini-modules, we can see that PID in CIGS results from sodium migration through absorber, most likely via grain boundaries. Potassium concentration distributions show little change when adding a voltage bias to a temperature and humidity stress. This suggests doping with other large alkali ions, such as cesium and rubidium, rather than sodium can increase the PID resistance of CIGS modules.

14 SOLAR ENERGY↗

Large-Area Material and Junction Damage in c–Si Solar Cells by Potential-Induced Degradation

This paper reports a new potential-induced degradation (PID) mechanism for crystalline silicon (c-Si), where Na diffuses everywhere and causes large-area material and junction degradation with point defects. Multiple characterization techniques are combined - Kelvin probe force microscopy, electron-beam induced current, dark lock-in thermography, transmission electron microscopy, time-of-flight secondary-ion mass spectrometry, and microwave photoconductance decay - as well as density functional theory (DFT) calculations. These characterization techniques and theoretical calculations are complementary in various aspects of a material's chemical, structural, electrical, and optoelectrical nature, as well as in atomic, nanometer, micrometer, millimeter, and cell and module scales. All results point consistently to a new discovery: substantial large-area deterioration of materials and junctions play a major role in c-Si PID (in addition to the previously reported local shunting defect caused by Na diffusion to planar defects). Furthermore, this new finding reveals a key PID component and leads to a new strategy for tailoring c-Si photovoltaics to ultimately resolve the PID issue.

14 SOLAR ENERGY↗

Analysis of Potential-Induced Degradation in Soda-Lime Glass and Borosilicate-Glass Cu(In,Ga)Se 2 Samples

In this study, potential-induced degradation (PID) is investigated in small-size Cu(In,Ga)Se 2 (CIGS) submodules of individual cells. Samples with conventional soda-lime glass (SLG) and low-alkaline glass (borosilicate glass, BSG) were analyzed applying positive and negative 1000 V bias at 85 degrees C and low relative humidity after a heat-soaking phase. During the heat-soaking phase, BSG samples showed degradation, with variations in their dark current-voltage (I-V) curve parameters compared with the stability of SLG samples. During the PID stress phase, back-grounded SLG samples with -1000 V applied to the cell experienced fast degradation, with complete failure in 25 h, whereas, BSG samples only showed changes because of the dark heat environment. When grounded on their front face, SLG samples remained stable during more than 150 h of PID testing, beginning degradation after longer applications of stress. The analysis of the dark I-V curves of SLG samples through the single-diode model showed that an increase in saturation current J 0 occurs first, attributed to Na + ions migrating into the CdS/ZnO layer; later, a decrease in shunt resistance occurs. Lastly, the application of the model in BSG samples showed an increase in series resistance evaluated at 25 degrees C. When the bias is reversed, SLG samples gradually recover their performance.

14 SOLAR ENERGY↗

Electrochemical mechanisms of leakage-current-enhanced delamination and corrosion in Si photovoltaic modules

This paper analyzes the mechanisms for corrosion and delamination observed in Si photovoltaic modules subjected to high temperature and humidity with a negative-ground bias testing. Based on the thermodynamic data, the ionic component of the leakage current causes reduction reactions of water on the cathodic metallization, producing hydrogen gas and hydroxide ions. Ag fingers are strong catalysts for this reduction reaction compared to other materials used in solar cells and can be the initiation sites of corrosion and delamination caused by the electrochemical reactions. The produced hydrogen gas accumulates inside the module potentially producing a high gas pressure that can promote delamination, which is often preferentially initiated on metallization where the adhesion strength is lower [1], [2], [3]. The local basicity near the metal surface increases due to the hydroxide ion generation. Thus, the environment inside the encapsulant can be alkaline despite the presence of acetic acid decomposition products from the encapsulant. Corrosion of materials such as Si used in solar cells occurs and the extent depends on their corrosion resistance to the alkaline solution. This suggests that corrosion and delamination are interactive and promote the formation and propagation of one another.

14 SOLAR ENERGY↗

Potential-Induced Degradation of Cu(In,Ga)Se 2 Solar Cells: Alkali Metal Drift and Diffusion Effects

Potential-induced degradation (PID) of photovoltaic modules is due to transport of alkali metal ions (Na + ) from the soda-lime glass (SLG) into the semiconductors. For the most efficient polycrystalline absorbers, Na and K in the Cu(In,Ga)(Se,S) 2 (CIGS) absorber often benefit performance, so a more detailed mechanism for PID is needed. To that end, CIGS solar cells have been encapsulated, stressed with high voltage, and cored to extract the active regions for characterization. SLG substrates led to 14.9% efficiency on average, which reduced to 0% after 25 h of -1000 V bias. This was accompanied by increased Na in the CIGS layer, particularly at the buffer interface, as well as decreased carrier concentrations. On the other hand, borosilicate glass substrates with low Na and high K content led to 13.6% efficiency on average, which only reduced to 12.1% after 25 h of stress. This was accompanied by slightly increased K content in the CIGS layer. As K has led to recent world record efficiency CIGS devices, understanding Na and K similarities and differences may help to enhance initial efficiency and reduce PID.

14 SOLAR ENERGY↗

Quantitative Electroluminescence Imaging Analysis for Performance Estimation of PID-Influenced PV Modules

An empirical method for estimating relative power losses caused by potential-induced degradation (PID) for p-type solar cells and modules using quantitative electroluminescence (EL) analysis (QELA) is presented. First, EL images are corrected for camera- and perspective distortion. The relative power loss map is then calculated from the logarithmic ratio of two EL images, taken either before and after PID degradation or at different applied currents. Only the cell average of the resulting power loss map is evaluated. The highest power loss across each string is averaged to obtain the overall power loss. Consequently, for modules with three strings, three cells are averaged. The resulting power loss depends on the current applied. The conversion to equivalent irradiance allows for comparison of measured and estimated device performance. The analysis of roughly 2000 EL images and related current-voltage (I-V) curves indicates a good agreement between flash-test-measured and performance estimated using QELA. A relative root mean square error of 1-3% can be achieved.

14 SOLAR ENERGY↗

Investigation of the Impact of Illumination on the Polarization-Type Potential-Induced Degradation of Crystalline Silicon Photovoltaic Modules

Accelerated potential-induced degradation (PID) testing of photovoltaic modules is conventionally conducted in the dark and at high temperature and humidity levels without considering the influence of illumination. This study investigates the impact of illumination on the polarization-type PID (PID-p) on two different types of encapsulated (glass/backsheet) crystalline silicon solar cells: 1) n-type bifacial passivated emitter rear totally diffused (the front side is facing glass and PID-stressed); and 2) p-type bifacial passivated emitter and rear cell (the rear side is facing glass and PID-stressed). The samples are stressed under the conditions of -1000 V, 40 degrees C, and 40% relative humidity and at different irradiance levels (xenon lamps). While the type-A modules show no reduction in PID-p sensitivity under illumination up to 800 W/m 2 , PID-p in the type-B modules is arrested by the light at an irradiance level as low as 10 W/m 2 . Furthermore, PID-degraded type-B modules (degradation induced in the dark) exhibit a rapid recovery (full recovery in 20 min) upon exposure to light (40 W/m 2 ). External quantum efficiency measurements on the type-B modules show that ultraviolet from 300 to 400 nm is mainly responsible for the fast recovery.

14 SOLAR ENERGY↗

Enabling reliability assessments of pre-commercial perovskite photovoltaics with lessons learned from industrial standards [Enabling reliability of pre-commercial perovskite photovoltaics with lessons learned from industrial standards]

Here, photovoltaic modules are expected to operate in the field for more than 25 years, so reliability assessment is critical for the commercialization of new photovoltaic technologies. In early development stages, understanding and addressing the device degradation mechanisms are the priorities. However, any technology targeting large-scale deployment must eventually pass industry-standard qualification tests and undergo reliability testing to validate the module lifetime. In this Perspective, we review the methodologies used to assess the reliability of established photovoltaics technologies and to develop standardized qualification tests. We present the stress factors and stress levels for degradation mechanisms currently identified in pre-commercial perovskite devices, along with engineering concepts for mitigation of those degradation modes. Recommendations for complete and transparent reporting of stability tests are given, to facilitate future inter-laboratory comparisons and to further the understanding of field-relevant degradation mechanisms, which will benefit the development of accelerated stress tests.

14 SOLAR ENERGY↗

Elucidating potential-induced degradation in bifacial PERC silicon photovoltaic modules

This paper elucidates the behavior and underlying mechanism of potential-induced degradation (PID) on the rear side of p-type monocrystalline silicon bifacial passivated emitter and rear cell (PERC) photovoltaic modules. At 50 degrees C, 30% relative humidity, and -1000 V bias to the solar cells with aluminium foil on the rear glass surface, the rear-side performance of bifacial PERC modules at standard testing conditions degraded dramatically after 40 hours with a 40.4%, 36.2%, and 7.2% loss in maximum power (Pmpp), short-circuit current (Isc), and open-circuit voltage (Voc), respectively. The front-side standard testing condition performance, on the other hand, showed less degradation; Pmpp, Isc, and Voc dropped by 12.0%, 5.2%, and 5.3%, respectively. However, negligible degradation was observed when the solar cells were positively biased. Based on I-V characteristics, electroluminescence, external quantum efficiency measurements, and the effective minority-carrier lifetime simulation, the efficiency loss is shown to be caused by the surface polarization effect; positive charges are attracted to the passivation/antireflection stack on the rear surface and reduce its field effect passivation performance. Extended PID testing to 100 hours showed an increase in device performances (relative to 40 hours) due to the formation of an inversion layer along the rear surface. In addition, replacing ethylene-vinyl acetate copolymer with polyolefin elastomer films significantly slows down the progression of PID, whereas a glass/transparent backsheet design effectively protects the rear side of bifacial PERC modules from PID. Furthermore, PID on the rear side of bifacial PERC modules is fully recoverable, and light greatly promotes recovery of the observed PID.

14 SOLAR ENERGY↗

Investigating PID shunting in polycrystalline silicon modules via multiscale, multitechnique characterization

We investigated the potential-induced degradation (PID) shunting mechanism in multicrystalline-silicon photovoltaic modules by using a multiscale, multitechnique characterization approach. Both field-stressed modules and laboratory-stressed mini modules were studied. We used photoluminescence, electroluminescence, and dark lock-in thermography imaging to identify degraded areas at the module scale. Small samples were then removed from degraded areas, laser marked, and imaged by scanning electron microscopy. We used simultaneous electron-beam induced current imaging and focused ion beam milling to mark around PID shunts for chemical analysis by time-of-flight secondary-ion mass spectrometry or to isolate individual shunt defects for transmission electron microscopy and atom-probe tomography analysis. By spanning a range of 10 orders of magnitude in size, this approach enabled us to investigate the root-cause mechanisms for PID shunting. We observed a direct correlation between recombination active shunts and sodium content. The sodium content in shunted areas peaks at the SiNX/Si interface and is consistently observed at a concentration of 0.1% to 2% in shunted areas. Analysis of samples subjected to PID recovery, either activated by electron beam or thermal effects only, reveals that recovery of isolated shunts correlates with diffusion of sodium out of the structural defects to the silicon surface. We observed the role of oxygen and chlorine in PID shunting and found that those species - although sometimes present in structural defects where PID shunting was observed - do not play a consistent role in PID shunting.

14 SOLAR ENERGY↗

Imaging, microscopic analysis, and modeling of a CdTe module degraded by heat and light

Photoluminescence (PL), electroluminescence (EL), and dark lock-in thermography are collected during stressing of a CdTe module under one-Sun light at an elevated temperature of 100 degrees C. The PL imaging system is simple and economical. The PL images show differing degrees of degradation across the module and are less sensitive to effects of shunting and resistance that appear on the EL images. Regions of varying degradation are chosen based on avoiding pre-existing shunt defects. These regions are evaluated using time-of-flight secondary ion-mass spectrometry and Kelvin probe force microscopy. Reduced PL intensity correlates to increased Cu concentration at the front interface. Numerical modeling and measurements agree that the increased Cu concentration at the junction also correlates to a reduced space charge region.

14 SOLAR ENERGY↗

A status review of photovoltaic power conversion equipment reliability, safety, and quality assurance protocols

Data indicate that the inverter is the element of the photovoltaic plant that has the highest number of service calls and the greatest operation and maintenance cost burden. This paper describes the projects and relevant background needed in developing design qualification standards that would serve to establish a minimum level of reliability, along with a review of photovoltaic inverter quality and safety standards, most of which are in their infancy. We compare stresses and levels for accelerated testing of inverters proposed in the standard drafts, and those proposed by manufacturers and purchasers of inverters. We also review bases for the methods, stress types, and stress levels for durability testing of key inverter components. Many of the test protocols appear to need more comprehensive inclusion of stress factors existing in the natural environment such as wind driven rain, dust, and grid disturbances. Further understanding of how temperature, humidity ingress, and voltage bias affect the inverters and their components is also required. We provide data indicating inconsistent quality of the inverters and the durability of components leading to greater cost for the photovoltaic plant operator. Accordingly, the recommendation for data collection within quality standards for obtaining cost of ownership metrics is made. Design validation testing using realistic operation, environmental, and connection conditions, including under end-use field conditions with feedback for continuous improvement is recommended for inclusion within a quality standard.

14 SOLAR ENERGY↗

Failure Analysis to Identify Thermal Runaway of Bypass Diodes in Fielded Modules

We studied a bypass diode recuperated from fielded modules in a rooftop installation to determine the failure mechanism. The field-failed diode showed similar characteristics to thermal runaway, specifically X-ray tomography evidence of migrated metal. We also observed burn marks on the silicon surface like those lab-stressed for thermal runaway. Reaction products are more soluble than silicon and the surface is oxygen rich.

14 SOLAR ENERGY↗

Further Studies on the Effect of SiN x Refractive Index and Emitter Sheet Resistance on Potential-Induced Degradation

We present the impacts of silicon nitride (SiNx) antireflection coating refractive index and emitter sheet resistance on potential-induced degradation of the shunting type (PID-s). Previously, it has been shown that the cell becomes more PID-s-susceptible as the refractive index decreases or the emitter sheet resistance increases. To verify the effect of refractive index on PID-s, we fabricated cells with varying SiN x refractive index (1.87, 1.94, 2.05) on typical p-type base solar cells with ~60 Ω/sq emitters. However, none of these cells showed output power degradation, regardless of the refractive index. Further investigation of the emitter showed that the PID-s was suppressed at ~60 Ω/sq due to the extremely high surface phosphorus concentration (6 x 10 21 cm -3 ), as measured by secondary ion mass spectrometry. Furthermore, PID-s was observed on cells possessing a high emitter sheet resistance (~80 Ω/sq). In conclusion, the emitter surface phosphorus concentration plays an important role in determining PID-s susceptibility.

14 SOLAR ENERGY↗

Potential-induced degradation in photovoltaic modules: a critical review

Potential-induced degradation (PID) has received considerable attention in recent years due to its detrimental impact on photovoltaic (PV) module performance under field conditions. Both crystalline silicon (c-Si) and thin-film PV modules are susceptible to PID. While extensive studies have already been conducted in this area, the understanding of the PID phenomena is still incomplete and it remains a major problem in the PV industry. Herein, a critical review of the available literature is given to serve as a one-stop source for understanding the current status of PID research. This article also aims to provide an overview of future research paths to address PID-related issues. This paper consists of three parts. In the first part, the modelling of leakage current paths in the module package is discussed. The PID mechanisms in both c-Si and thin-film PV modules are also comprehensively reviewed. The second part summarizes various test methods to evaluate PV modules for PID. The last part focuses on studies related to PID in the omnipresent p-type c-Si PV modules. The dependence of temperature, humidity and voltage on the progression of PID is examined. Preventive measures against PID at the cell, module and system levels are illustrated. Moreover, PID recovery in standard p-type c-Si PV modules is also studied. Most of the findings from p-type c-Si PV modules are also applicable to other PV module technologies.

14 SOLAR ENERGY↗

Assessing the Causes of Encapsulant Delamination in PV Modules

Delamination of the encapsulant is one of the most prevalent PV module field failures. This paper will present examples of various types of delaminations that have been observed in the field. It will then discuss the development of accelerated stress tests designed to duplicate those field failures and thus provide tools for avoiding them in the future.

14 SOLAR ENERGY↗

Development of Cu(In,Ga)Se2 Test Coupons for Potential Induced Degradation Studies

We report on the design, fabrication and accelerated testing of fully encapsulated small area coupons (approximately 7.5cm x 7.5 cm) for the purpose of researching potential induced degradation in Cu(In, Ga)Se2 based PV modules. The fabrication of these coupons enables the study of the solar cells and the materials used in PV module manufacturing such as top and bottom glass covers of different composition (soda-lime glass, high temperature glass, alkaline-free glass, etc), plastic-based top covers, ethylene vinyl acetate and edge seal encapsulation materials. The coupons can also be used to emulate framed and frameless modules that utilize either monolithically interconnected modules or singular cell type of modules. The design of the coupons, their fabrication, the materials used and their testing for 1000 hours under 85 degrees C and 85% RH conditions are presented.

14 SOLAR ENERGY↗