Engineering topics
Gul, R
Publications and source records attributed to Gul, R.
Point Defects in CdZnTe Crystals Grown by Different Techniques
We studied, by current deep-level transient spectroscopy (I-DLTS), point defects in CdZnTe detectors grown by different techniques. We identified 12 different traps with energy levels from 7 meV to 1.1 eV. Although the levels of most of the identified defects were independent of the crystal growth techniques, nevertheless there were some associated differences in the traps energies and densities.
Effect of Extended Defects in Planar and Pixelated CdZnTe Detectors
We evaluated a spectroscopy-grade 15 x 15 x 7 mm{sup 3} CdZnTe (CZT) crystal with a high {mu}{tau}-product, > 10{sup -2} cm{sup 2}/V, but impaired by microscopic extended defects, such as walls of dislocations, low-angle and sub-grain boundaries, and Te inclusions. First, we evaluated a planar detector fabricated from this crystal using a Microscale X-ray Detector Mapping (MXDM) technique. Then, we fabricated from the same crystal a pixel detector to study local non-uniformities of the electric field. The measured X-ray response maps confirmed the presence of non-uniformities in the charge transport, and they showed that the global- and local-distortions of the internal E-field correlated to the extended defects and space-charge buildup on the side surfaces.
Effect of Te Inclusions in CdZnTe Crystals at Different Temperatures
CdZnTe crystals often exhibit nonuniformities due to the presence of Te inclusions and dislocations. High concentrations of such defects in these crystals generally entail severe charge-trapping, a major problem in ensuring the device's satisfactory performance. In this study, we employed a high-intensity, high-spatial-resolution synchrotron x-ray beam as the ideal tool to generate charges by focusing it over the large Te inclusions, and then observing the carrier's response at room- and at low-temperatures. A high spatial 5-{micro}m resolution raster scan revealed the fine details of the presence of extended defects, like Te inclusions and dislocations in the CdZnTe crystals. A noticeable change was observed in the efficiency of electron charge collection at low temperature (1 C), but it was hardly altered at room-temperature.
Defect Levels of Indium-doped CdMnTe Crystals
Using photoluminescence (PL) and current deep-level transient spectroscopy (I-DLTS), we investigated the electronic defects of indium-doped detector-grade CdMnTe:In (CMT:In) crystals grown by the vertical Bridgman method. We similarly analyzed CdZnTe:In (CZT:In) and undoped CdMnTe (CMT) crystals grown under the amount of same level of excess Te and/or indium doping level to detail the fundamental properties of the electronic defect structure more readily. Extended defects, existing in all the samples, were revealed by synchrotron white beam x-ray diffraction topography and scanning electron microscopy. The electronic structure of CMT is very similar to that of CZT, with shallow traps, A-centers, Cd vacancies, deep levels, and Te antisites. The 1.1-eV deep level, revealed by PL in earlier studies of CZT and CdTe, were attributed to dislocation-induced defects. In our I-DLTS measurements, the 1.1-eV traps showed different activation energies with applied bias voltage and an exponential dependence on the trap-filling time, which are typical characteristics of dislocation-induced defects. We propose a new defect-trap model for indium-doped CMT crystals.
Correlations Between Crystal Defects and Performance of CdZnTe Detectors
Poor crystallinity remains a major problem affecting the availability and cost of CdZnTe (CZT) detectors. Point defects are responsible for small gradual charge loss and correlated with the electron clouds' drift times, which allows electronic correction of the output signals to achieve high spectral-resolution even with large-volume CZT detectors. In contrast, extended defects causes significant charge losses, which typically are uncorrelated, and, thus, result in much greater fluctuations of the output signals that cannot be corrected. Although extended defects do not affect all the interaction events, their fraction rapidly increases with the crystal's thickness and volume. In this paper, we summarize our recent results from testing CZT material and detectors that emphasize the particular roles of two types of extended defects, and their contributions to the device's overall performance.
Hybrid Contacts for CZT Virtual Frisch-grid Detectors
In our previous design of virtual Frisch-grid CdZnTe (CZT) detectors, the charge drift-lines can be terminated at the side surfaces before the carriers reach the collecting anode; this results in a loss of signal from the interacting events near the detector's edges. Here, we describe our new design for the anode contact that reduces these edge effects by focusing the electric field towards the detectors' central axes. Four detectors were fabricated with the new hybrid anode contact, and their performances were evaluated and compared to those from the previous design for our virtual Frisch-grid detectors. The results obtained for all four showed similar improvement: therefore, we illustrate them with the findings from one detector.
An effect of the networks of the subgrain boundaries on spectral responses of thick CdZnTe detectors
CdZnTe (CZT) crystals used for nuclear-radiation detectors often contain high concentrations of subgrain boundaries and networks of poligonized dislocations that can significantly degrade the performance of semiconductor devices. These defects exist in all commercial CZT materials, regardless of their growth techniques and their vendor. We describe our new results from examining such detectors using IR transmission microscopy and white X-ray beam diffraction topography. We emphasize the roles on the devices performances of networks of subgrain boundaries with low dislocation densities, such as poligonized dislocations and mosaic structures. Specifically, we evaluated their effects on the gamma-ray responses of thick, >10 mm, CZT detectors. Our findings set the lower limit on the energy resolution of CZT detectors containing dense networks of subgrain boundaries, and walls of dislocations.
IMPROVEMENT OF CdMnTe DETECTOR PERFORMANCE BY MnTe PURIFICATION
Residual impurities in manganese (Mn) are a big obstacle to obtaining high-performance CdMnTe (CMT) X-ray and gamma-ray detectors. Generally, the zone-refining method is an effective way to improve the material's purity. In this work, we purified the MnTe compounds combining the zone-refining method with molten Te, which has a very high solubility for most impurities. We confirmed the improved purity of the material by glow-discharge mass spectrometry (GDMS). We also found that CMT crystals from a multiply-refined MnTe source, grown by the vertical Bridgman method, yielded better performing detectors.
Internal Electric Field Behavior of Cadmium Zinc Telluride Radiation Detectors Under High Carrier Injection
The behavior of the internal electric-field of nuclear-radiation detectors substantially affects the detector's performance. We investigated the distribution of the internal field in cadmium zinc telluride (CZT) detectors under high carrier injection. We noted the build-up of a space charge region near the cathode that produces a built-in field opposing the applied field. Its presence entails the collapse of the electric field in the rest of detector, other than the portion near the cathode. Such a space-charge region originates from serious hole-trapping in CZT. The device's operating temperature greatly affects the width of the space-charge region. With increasing temperature from 5 C to 35 C, its width expanded from about 1/6 to 1/2 of the total depth of the detector.
Array of virtual Frisch-grid CZT detectors with common cathode readout and pulse-height correction
We present our new results from testing 15-mm-long virtual Frisch-grid CdZnTe detectors with a common-cathode readout for correcting pulse-height distortions. The array employs parallelepiped-shaped CdZnTe (CZT) detectors of a large geometrical aspect ratio, with two planar contacts on the top and bottom surfaces (anode and cathode) and an additional shielding electrode on the crystal's sides to create the virtual Frisch-grid effect. We optimized the geometry of the device and improved its spectral response. We found that reducing to 5 mm the length of the shielding electrode placed next to the anode had no adverse effects on the device's performance. At the same time, this allowed corrections for electron loss by reading the cathode signals to obtain depth information.
Study on thermal annealing of cadmium zinc telluride (CZT) crystals
Cadmium Zinc Telluride (CZT) has attracted increasing interest with its promising potential as a room-temperature nuclear-radiation-detector material. However, different defects in CZT crystals, especially Te inclusions and dislocations, can degrade the performance of CZT detectors. Post-growth annealing is a good approach potentially to eliminate the deleterious influence of these defects. At Brookhaven National Laboratory (BNL), we built up different facilities for investigating post-growth annealing of CZT. Here, we report our latest experimental results. Cd-vapor annealing reduces the density of Te inclusions, while large temperature gradient promotes the migration of small-size Te inclusions. Simultaneously, the annealing lowers the density of dislocations. However, only-Cd-vapor annealing decreases the resistivity, possibly reflecting the introduction of extra Cd in the lattice. Subsequent Te-vapor annealing is needed to ensure the recovery of the resistivity after removing the Te inclusions.
Extended defects in as-grown CdZnTe
We characterized samples cut from different locations in as-grown CdZnTe (CZT) ingots, using Automated Infrared (IR) Transmission Microscopy and White Beam X-ray Diffraction Topography (WBXDT), to locate and identify the extended defects in them. Our goal was to define the distribution of these defects throughout the entire ingot and their effects on detectors’ performance as revealed by the pulse-height spectrum. We found the highest- and the lowest- concentration of Te inclusions, respectively, in the head and middle part of the ingot, which could serve as guidance in selecting samples. Crystals with high concentration of Te inclusions showed high leakage current and poor performance, because the accumulated charge loss around trapping centers associated with Te inclusions distorts the internal electric field, affects the carrier transport properties inside the crystal, and finally degrades the detector’s performance. In addition, other extended defects revealed by the WBXDT measurements severely reduced the detector’s performance, since they trap large numbers of electrons, leading to a low signal for the pulse-height spectrum, or none whatsoever. Finally, we fully correlated the detector’s performance with our information on the extended defects gained from both the IR- and the WBXDT-measurements.
Cadmium Manganese Telluride (Cd1-xMnxTe): A potential material for room-temperature radiation detectors
Cadmium Manganese Telluride (CdMnTe) recently emerged as a promising material for room-temperature X- and gamma-ray detectors. It offers several potential advantages over CdZnTe. Among them is its optimal tunable band gap ranging from 1.7-2.2 eV, and its relatively low (< 50%) content of Mn compared to that of Zn in CdZnTe that assures this favorable band-gap range. Another important asset is the segregation coefficient of Mn in CdTe that is approximately unity compared to 1.35 for Zn in CdZnTe, so ensuring the homogenous distribution of Mn throughout the ingot; hence, a large-volume stoichiometric yield is attained. However, some materials issues primarily related to the growth process impede the production of large, defect-free single crystals. The high bond-ionicity of CdMnTe entails a higher propensity to crystallize into a hexagonal structure rather than to adopt the expected zinc-blend structure, which is likely to generate twins in the crystals. In addition, bulk defects generate in the as-grown crystals due to the dearth of high-purity Mn, which yields a low-resistivity material. In this presentation, we report on our observations of such material defects in current CdMnTe materials, and our evaluation of its potential as an alternative detector material to the well-known CdZnTe detectors. We characterized the bulk defects of several indium- and vanadium-doped Cd1-xMnxTe crystals by using several advanced techniques, viz., micro-scale mapping, white-beam x-ray diffraction/reflection topography, and chemical etching. Thereafter, we fabricated some detectors from selected CdMnTe crystals, characterized their electrical properties, and tested their performance as room-temperature X- and gamma-ray detectors. Our experimental results indicate that CdMnTe materials could well prove to become a viable alternative in the near future.