Engineering Papers⌕ Search

Engineering topics

Fezzaa, Kamel

Publications and source records attributed to Fezzaa, Kamel.

At least 37 records · Page 2

In-Situ X-Ray Imaging High Strain Rate Compression of Laminate Al-Graphene Composite and Mechanical Property Characterization

Owing to the opaque nature of the laminated structures, traditional high-speed optical camera cannot be used to detect the dynamic process of sub-surface deformation. In this article, we report a study of using high speed X-ray imaging to study the high strain rate deformation in laminated Al structures. We used a Kolsky bar apparatus to apply dynamic compression and a high-speed synchrotron X-ray phase contrast imaging (PCI) setup to conduct the in situ X-ray imaging study. The in situ X-ray imaging captures the shock wave propagation in the laminated structures. After shock compression, we characterized the microstructures by using transmission electron microscopy (TEM), which demonstrates an increase of dislocation density. In conclusion, the micro-pillar compression tests show that the yield strength at 0.2% offset of laminated Al-graphene composite has a significant increase of 67%, from 30 to 50 MPa, compared to laminate Al after shock loading.

36 MATERIALS SCIENCE↗

Melt pool instability detection using coaxial photodiode system validated by in-situ X-ray imaging

A co-axial photodiode monitoring system with high temporal resolution has been integrated into a proven test bench enabling synchronized side-view high speed X-ray imaging of melt pool dynamics and top-view spectral emission characterization of the melt pool. Here, this setup enables direct observation of melt pool phenomena and correlation between the two monitoring systems which can be directly scaled to commercial systems. The work demonstrates a 92% detection rate in keyhole collapse phenomena related to defect generation in SLM. Furthermore, the impact of gas flow on monitoring signals is studied to understand the fundamental importance of gas flow in commercial systems.

36 MATERIALS SCIENCE↗

High-speed X-ray study of process dynamics caused by surface features during continuous-wave laser polishing

During high-speed X-ray imaging of laser surface polishing experiments of specimens of 316L stainless steel at Argonne National Lab's Advanced Photon Source, it was discovered that the induced keyhole changes shape and dimensions while crossing an engineered surface feature without altering process parameters. It was observed that the post-surface feature keyhole was deeper than that of the pre surface feature keyhole. Here, this work reports on the first in-situ observation of the effect of localized surface geometry on underlying melt pool behavior. This has implications for defect formation mechanisms during laser melting processes that rely on melt pool geometry.

42 ENGINEERING↗

Understanding process-microstructure-property relationships in laser powder bed fusion of non-spherical Ti-6Al-4V powder

Powder feedstock is a major cost driver in metal additive manufacturing (AM). Replacing the spherical powder with the cost-efficient non-spherical one can reduce the feedstock cost up to 50% and attract more interest to adopt AM in production and new alloy development. Here, for this paper, a comprehensive study was conducted to understand process-microstructure-property relationships in laser powder bed fusion of hydride-dehydride Ti-6Al-4V powder. We demonstrated that variation of laser scan speed had a significant impact on the grain structure, pore evolution and properties compared to laser power. Dynamic X-ray radiography showed that with decreasing scan speed at a constant laser power, a transition from conduction to keyhole mode laser processing occurred, in which a deeper melt pool at lower scan speed intensified texture. In other words, an increase in laser scan speed resulted in formation of the refined prior β grains with shape factor of ~5, lowering the anisotropy. Furthermore, the degree of variant selection was evaluated based on the analyzed texture as a function of laser power and scan speed. With increasing laser scan speed, the dominant α/α boundary type was altered from type 2 to 4 and the degree of variant selection was noticeably decreased. On the other hand, increasing laser power left the morphology of prior β grains, their size, and the dominant α/α boundary (type 4) unchanged, while the texture and anisotropy were intensified, and the degree of variant selection was slightly decreased. Finally, dependency of surface roughness and microhardness were discussed as a function of laser processing parameters.

variant selection↗

High frequency beam oscillation keyhole dynamics in laser melting revealed by in-situ x-ray imaging

The metal additive manufacturing industry is actively developing instruments and strategies to enable higher productivity, optimal build quality, and controllable as-built microstructure. A beam controlling technique, laser oscillation has shown potential in all these aspects in laser welding; however, few attempts have been made to understand the underlying physics of the oscillating keyholes/melt pools which are the prerequisites for these strategies to become a useful tool for laser-based additive manufacturing processes. Here, to address this gap, we utilized a synchrotron-based X-ray operando technique to image the dynamic keyhole oscillation in Ti-6Al-4V using a miniature powder bed fusion setup. We found good agreement between the experimental observations and simulations performed with a validated Lattice Boltzmann multiphysics model. The study revealed the continuous and periodic fluctuations in the characteristic keyhole parameters that are unique to the oscillating laser beam processing and responsible for the chevron pattern formation at solidification. In particular, despite the intrinsic longer-range fluctuation, the oscillating technique displayed potential for reducing keyhole instability, mitigating porosity formation, and altering surface topology. These insights on the oscillating keyhole dynamics can be useful for the future development and application of this technique.

36 MATERIALS SCIENCE↗

Machine learning–aided real-time detection of keyhole pore generation in laser powder bed fusion

Porosity defects are currently a major factor that hinders the widespread adoption of laser-based metal additive manufacturing technologies. One common porosity occurs when an unstable vapor depression zone (keyhole) forms because of excess laser energy input. With simultaneous high-speed synchrotron x-ray imaging and thermal imaging, coupled with multiphysics simulations, we discovered two types of keyhole oscillation in laser powder bed fusion of Ti-6Al-4V. Amplifying this understanding with machine learning, we developed an approach for detecting the stochastic keyhole porosity generation events with submillisecond temporal resolution and near-perfect prediction rate. Finally, the highly accurate data labeling enabled by operando x-ray imaging allowed us to demonstrate a facile and practical way to adopt our approach in commercial systems.

42 ENGINEERING↗

Vorticity-induced flow-focusing leads to bubble entrainment in an inkjet printhead: Synchrotron x-ray and volume-of-fluid visualizations

The oscillatory flows present in an inkjet printhead can lead to strong deformations of the air-liquid interface at the nozzle exit. Such deformations may lead to an inward directed air jet with bubble pinch-off and the subsequent entrainment of an air bubble, which is highly detrimental to the stability of inkjet printing. Understanding the mechanisms of bubble entrainment is therefore crucial to improving print stability. Here, in the present work, we use ultrafast x-ray phase-contrast imaging and direct numerical simulations based on the volume-of-fluid method to study the mechanisms underlying the bubble entrainment in a piezoacoustic printhead. We first demonstrate good agreement between experiments and numerics. We then show the different classes of bubble pinch-off obtained in experiments, and that those were also captured numerically. The numerical results are then used to show that the baroclinic torque, which is generated at the gas-liquid interface due to the misalignment of density and pressure gradients, results in a flow-focusing effect that drives the formation of the air jet from which a bubble can pinch off.

42 ENGINEERING↗

Nanoparticle-enabled increase of energy efficiency during laser metal additive manufacturing

The low energy efficiency of the laser metal additive manufacturing (AM) process is a potential sustainability concern for large-scale industrial production. Explicit investigation of the energy efficiency for laser melting requires the direct characterization of melt pool dimension and vapor depression, which is very difficult due to the opaque nature of the molten metal. Here we report the direct observation and quantification of effects of the TiC nanoparticles on the vapor depression and melt pool formation during laser powder bed fusion (LPBF) of Al6061 by in-situ high-speed high-energy x-ray imaging. Based on the quantification results, we calculated the laser melting energy efficiency (defined here as the ratio of the energy needed to melt the material to the energy delivered by the laser beam) with and without TiC nanoparticles during LPBF of Al6061. Here the results show that adding TiC nanoparticles into Al6061 leads to a significant increase of laser melting energy efficiency (114% increase on average, 521% increase under 312 W laser power, 0.4 m/s scan speed). Systematic property measurement, simulation, and x-ray imaging studies enable us, for the first time, to identify that three mechanisms work together to enhance the laser melting energy efficiency: (1) adding TiC nanoparticles increases the absorptivity; (2) adding TiC nanoparticles decreases the thermal conductivity, and (3) adding TiC nanoparticles enables the initiation of vapor depression and multiple reflection at lower laser power (i.e., lowers the laser power threshold for keyholing). The method and mechanisms of using TiC nanoparticles to increase the laser melting energy efficiency during LPBF of Al6061 we reported here may guide the development of feedstock materials for more energy efficient laser metal AM.

36 MATERIALS SCIENCE↗

Laser melting modes in metal powder bed fusion additive manufacturing

In laser powder bed fusion additive manufacturing of metals, extreme thermal conditions create many highly dynamic physical phenomena such as vaporization and recoil, Marangoni convection, and protrusion and keyhole instability. Collectively however, the full set of phenomena is too complicated for practical applications and, in reality, the melting modes are used as a guideline for printing. With increasing local material temperature beyond the boiling point, the mode can change from conduction to keyhole. These mode designations ignore laser-matter interaction details but in many cases are adequate to determine the approximate microstructures and hence the properties of the build. To date, no consistent, common, and coherent definitions have been agreed upon because of historic limitations in melt pool and vapor depression morphology measurements. Here, we distinguish process-based definitions of different melting modes from those based on postmortem evidence. The latter are mainly derived from the transverse cross-sections of the fusion zone, whereas the former come directly from time-resolved x-ray imaging of melt pool and vapor depression morphologies. These process-based definitions are more strict and physically sound, and they offer new guidelines for laser additive manufacturing practices and create new research directions. Further, we highlight the significance of the keyhole, which substantially enhances the laser energy absorption by the melt pool. Recent studies strongly suggest that stable-keyhole laser melting enables efficient, sustainable, and robust additive manufacturing. The realization of this scenario demands the development of multiphysics models, signal translations from morphology to other feasible signals, and in-process metrology across platforms and scales.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Resolving the Martensitic Transformation in Q&P Steels In-Situ at Dynamic Strain Rates Using Synchrotron X-ray Diffraction

Herein the dynamic deformation response of two quenching and partitioning (Q&P) steels was investigated using a high strain rate tension pressure bar and in-situ synchrotron radiography and diffraction. This allowed for concurrent measurements of the martensitic transformation, the elastic strains/stresses on the martensite and ferrite, and the bulk mechanical behavior. The steel with the greater fraction of ferrite exhibited greater ductility and lower strength, suggesting that dislocation slip in ferrite enhanced the deformability. Meanwhile, the kinetics of the martensitic transformation appeared similar for both steels, although the steel with a greater ferrite fraction retained more austenite in the neck after fracture.

36 MATERIALS SCIENCE↗

Controlling melt flow by nanoparticles to eliminate surface wave induced surface fluctuation

The high surface roughness is one of the major challenges encountered in laser metal additive manufacturing (AM) processes, which is closely related to the melt flow behavior. However, how to control the melt flow in laser metal AM processes to improve surface finish is unknown. Here we reveal the effects of nanoparticles on melt flow behavior at every location of melt pool during laser metal AM process for the first time using Al6061 + TiC nanoparticles system and achieve significant improvement of surface finish by using TiC nanoparticles to control the melt flow and damp the surface wave. Based on the in-situ x-ray imaging observation, the surface wave is fully damped after adding TiC nanoparticles, compared with only 56% damping without nanoparticles during LPBF of Al6061. Our in-depth in-situ x-ray imaging analysis and viscosity measurement enable us to identify that nanoparticle-induced increase of viscosity causes the fully damping of the surface wave by (1) increasing the internal fluid friction for more efficient wave amplitude reduction, (2) controlling the melt flow to increase the surface wave number, (3) controlling the melt flow to increase the wave damping time. Furthermore, we also quantified the relative contributions of increasing fluid friction, increasing wave number, and increasing damping time to wave damping, which account for 61%, 25%, and 14%, respectively. Furthermore, our research provides the mechanisms and potential method to address the surface finish challenge in laser metal AM processes.

36 MATERIALS SCIENCE↗

In situ melt pool measurements for laser powder bed fusion using multi sensing and correlation analysis

Laser powder bed fusion is a promising technology for local deposition and microstructure control, but it suffers from defects such as delamination and porosity due to the lack of understanding of melt pool dynamics. To study the fundamental behavior of the melt pool, both geometric and thermal sensing with high spatial and temporal resolutions are necessary. This work applies and integrates three advanced sensing technologies: synchrotron X-ray imaging, high-speed IR camera, and high-spatial-resolution IR camera to characterize the evolution of the melt pool shape, keyhole, vapor plume, and thermal evolution in Ti–6Al–4V and 410 stainless steel spot melt cases. Aside from presenting the sensing capability, this paper develops an effective algorithm for high-speed X-ray imaging data to identify melt pool geometries accurately. Preprocessing methods are also implemented for the IR data to estimate the emissivity value and extrapolate the saturated pixels. Quantifications on boundary velocities, melt pool dimensions, thermal gradients, and cooling rates are performed, enabling future comprehensive melt pool dynamics and microstructure analysis. The study discovers a strong correlation between the thermal and X-ray data, demonstrating the feasibility of using relatively cheap IR cameras to predict features that currently can only be captured using costly synchrotron X-ray imaging. Such correlation can be used for future thermal-based melt pool control and model validation.

47 OTHER INSTRUMENTATION↗

Phase Contrast X‐Ray Imaging of the Collapse of an Engineered Void in Single‐Crystal HMX

Abstract Imaging the collapse of a single void that creates a hot spot initiation site in an otherwise defect‐free explosive is challenging given the spatial and temporal scales involved in explosive systems. This work presents our attempt to examine a single hot spot mode (void collapse) in single‐crystal octahydro‐l,3,5,7‐tetranitro‐l,3,5,7‐tetrazocine (HMX) embedded in Sylgard. The hot spot heating mechanisms involved with pore collapse include adiabatic heating, jetting, and viscoplastic dissipation. Quantifying the dynamics of a pore collapse is a crucial step to understanding which mechanisms dominate during ignition events. Our experiments were conducted with a single‐stage, light‐gas gun at Argonne National Laboratory's Advanced Photon Source, applying the phase contrast imaging technique while collecting high‐speed video. The details of HMX single crystal production, defect (pore) engineering, and sample construction, along with experimental results are presented here. These results demonstrate that detailed collapse dynamics can be obtained from homogeneous, single‐crystal explosives with this approach. Qualitative comparisons are made with simulation data which show good agreement in the transition between a quasi‐symmetric pore collapse and an asymmetric collapse with jetting across the pore as measured with normalized pore area and pore circularity.

42 ENGINEERING↗

In Situ X-ray Radiography and Computational Modeling to Predict Grain Morphology in $\beta$-Titanium during Simulated Additive Manufacturing

The continued development of metal additive manufacturing (AM) has expanded the engineering metallic alloys for which these processes may be applied, including beta-titanium alloys with desirable strength-to-density ratios. To understand the response of beta-titanium alloys to AM processing, solidification and microstructure evolution needs to be investigated. In particular, thermal gradients (Gs) and solidification velocities (Vs) experienced during AM are needed to link processing to microstructure development, including the columnar-to-equiaxed transition (CET). In this work, in situ synchrotron X-ray radiography of the beta-titanium alloy Ti-10V-2Fe-3Al (wt.%) (Ti-1023) during simulated laser-powder bed fusion (L-PBF) was performed at the Advanced Photon Source at Argonne National Laboratory, allowing for direct determination of Vs. Two different computational modeling tools, SYSWELD and FLOW-3D, were utilized to investigate the solidification conditions of spot and raster melt scenarios. The predicted Vs obtained from both pieces of computational software exhibited good agreement with those obtained from in situ synchrotron X-ray radiography measurements. The model that accounted for fluid flow also showed the ability to predict trends unobservable in the in situ synchrotron X-ray radiography, but are known to occur during rapid solidification. A CET model for Ti-1023 was also developed using the Kurz–Giovanola–Trivedi model, which allowed modeled Gs and Vs to be compared in the context of predicted grain morphologies. Both pieces of software were in agreement for morphology predictions of spot-melts, but drastically differed for raster predictions. The discrepancy is attributable to the difference in accounting for fluid flow, resulting in magnitude-different values of Gs for similar Vs.

36 MATERIALS SCIENCE↗

Mitigating keyhole pore formation by nanoparticles during laser powder bed fusion additive manufacturing

Keyhole pore formation is one of the most detrimental subsurface defects in the laser metal additive manufacturing process. However, effective ways to mitigate keyhole pore formation beyond tuning laser processing conditions during keyhole mode laser melting are still lacking. Here we report a novel approach to mitigate keyhole pore formation during laser powder bed fusion (LPBF) process by using stable nanoparticles. The critical keyhole depth for keyhole pore generation (i.e., the largest keyhole depth without keyhole pore formation) during LPBF of Al6061 increases from 246 µm to 454 µm (85% increase) after adding TiC nanoparticles. In-depth x-ray imaging studies and thermo-fluid dynamics simulation enable us to identify that two mechanisms work together to mitigate keyhole pore generation: (1) adding nanoparticles prevents the keyhole from collapsing by increasing the liquid viscosity to impede the protrusion development; (2) adding nanoparticles slows down the keyhole pore movement by increasing the liquid viscosity, resulting in the recapturing of the pore by the keyhole. We further demonstrate that adding TiC nanoparticles can also eliminate the keyhole fluctuation induced keyhole pore during LPBF of Al6061. Our research provides a potential way to mitigate keyhole pore formation for defect lean metal additive manufacturing.