Elongated Fullerene Unlocks Oxygen-Resistant Perovskite Solar Minimodules

State-of-the-art encapsulation cannot prevent the permeation of oxygen into perovskite solar cells (PSCs). Here, we report the finding that p-i-n structured PSCs degrade quickly under oxygen exposure. Oxidation of C60, rather than perovskites, dominates the degradation. Chemical absorption of oxygen by C60 is identified, which impairs its electron transport property. We modify the electron transport layers to address the instability under oxygen exposure. The elongated fullerene C70 is found to react with oxygen orders of magnitude slower than C60. In combination with a compact SnO2 buffer fabricated by atomic layer deposition, which can slow down the oxygen diffusion, the resulting unencapsulated PSCs with C70 retained 90% of their initial efficiency after 1-sun illumination in pure oxygen for 1,200 h at 70 degrees C, improving stability by hundreds of times. Testing of unencapsulated perovskite minimodules of different perovskite compositions with C70 gives extrapolated lifetimes of 17-41 years at 50 degrees C.

14 SOLAR ENERGY

C60-Based Ionic Salt Electron Shuttle for High-Performance Inverted Perovskite Solar Modules

Although C60 is usually the electron transport layer (ETL) in inverted perovskite solar cells, its molecular nature of C60 leads to weak interfaces that lead to non-ideal interfacial electronic and mechanical degradation. Here, we synthesized an ionic salt from C60, 4-(1',5'-dihydro-1'-methyl-2'H-[5,6] fullereno-C60-Ih-[1,9-c]pyrrol-2'-yl) phenylmethanaminium chloride (CPMAC), and used it as the electron shuttle in inverted PSCs. The CH2-NH3+ head group in the CPMA cation improved the ETL interface and the ionic nature enhanced the packing, leading to ~3-fold increase in the interfacial toughness compared to C60. Using CPMAC, we obtained ~26% power conversion efficiencies (PCEs) with ~2% degradation after 2,100 hours of 1-sun operation at 65degrees C. For minimodules (four subcells, 6 centimeters square), we achieved the PCE of ~23% with <9% degradation after 2,200 hours of operation at 55degrees C.

14 SOLAR ENERGY