Advanced Manufacturing and Materials Technologies for Gasification
Presented by LRST at the 2020 Gasification Project Review Meeting, 9/2
Engineering topics
Publications and source records attributed to Dogan, Omer.
Presented by LRST at the 2020 Gasification Project Review Meeting, 9/2
Presented by NETL at TMS 2020, 02/20
Presented by NETL at TMS Annual Meeting 2020, 02/20
Presented by NETL at UK-US Collaboration on Fossil Energy R&D Workshop, 09/19
Presented by NETL at UK-US Collaboration on Fossil Energy R&D Workshop, 04/19
<span>US-UK Phase 3 Task 1 Oxidation in Supercritical Fluids (NETL) presented by NETL at the US-UK Phase 3 Workshop April 8-9, 2019 in Pittsburgh, PA</span>
Explore the source record for details and available documents.
Presented by NETL at MS&T18, 10/18
Presented by NETL at MS&T, 10/18
Explore the source record for details and available documents.
We show that considerable structural transformations occur at a Ni alloy surface during the transient stages of high-temperature oxidation. This was demonstrated by exposing the alloy to high-temperature CO 2 for short times at both atmospheric and supercritical pressures. A protective Cr-rich oxide layer formed after only 5 min at 700 °C and persisted for longer exposures up to 500 h. Voids formed and grew over time by the condensation of metal vacancies generated during oxidation, while the alloy surface recrystallized after sufficient oxidation had occurred. The oxygen potential established at the oxide/alloy interface led to oxidation along the newly formed grain boundaries as well as adjacent to and inside of the voids. Al, the most stable oxide-former and present at low concentration in the alloy, was preferentially oxidized in these regions. Furthermore, the results provide an improved understanding of the internal oxidation of Al and its role in enhancing scale adhesion for this class of Ni alloys.
Presented by NETL at The 6th International Symposium - sCO2 Power Cycles 2018, 03/18
This presentation briefly describes the R&D efforts on supercritical CO2 (sCO2) power cycles currently being performed at NETL's Research & Innovation Center. R&D is ongoing in five main areas: Aerothermal/Heat Transfer, Oxy-combustion, sCO2 Materials, Dynamic Cycle Modeling, and Techno-economic Analyses. This presentation was delivered at the 2017 sCO2 Summit in Albuquerque, NM, on 11/15/17.
Presented by NETL at 70th Annual Meeting of the APS Division of Fluid Dynamics, 11/17
<span>Presented by NETL at Pacific Northwest Chapter of AVS Annual Meeting, 09/17</span>
Presented by NETL at 2018 TMS Annual Meeting & Exhibition, 03/18
In order to understand issues with corrosion of heat exchanger materials in direct supercritical carbon dioxide (sCO 2 ) power cycles, a series of autoclave exposure experiments and electrochemical experiments have been conducted. Corrosion behaviors of 347H stainless steel and P91 martensitic-ferrtic steel in sCO 2 environment have been compared. In autoclave exposure tests performed at 50°C- 245°C and 80 bar. Mass change measurements, surface characterization, and corrosion product analysis have been conducted to understand the corrosion behavior of steels in sCO 2 containing H 2 O and O 2 . Electrochemical tests performed at room temperature and 50°C, a simulation environment of water condensation phase with dissolved CO 2 was prepared to evaluate the corrosion resistance of materials. From both types of experiments, generally 347H showed higher corrosion resistance than P91.