Engineering Papers⌕ Search

Engineering topics

Daehn, Glenn

Publications and source records attributed to Daehn, Glenn.

(Project 18-15531) Repair and Mitigation of Chloride-Induced Pitting and Chloride-Induced Stress Corrosion Cracking in Used Spent Nuclear Fuel Dry Cask Canister Materials (Final Technical Report)

Several experimental techniques were utilized to understand the corrosion and SCC performance of possible techniques for repairing cracks and pits in SS304 utilized for dry cask storage of spent nuclear fuel. The repairs examined included cold spray, FSW, soldering, and VFAW. The corrosion and SCC assessment techniques utilized for comparing repairs against the base material were 4-pt bending SCC testing in boiling MgCl 2 at stress levels between 0 MPa and 350 MPa, immersion testing in 40% RH brine solution meant to mimic a service-like environment, SSRT SCC testing in 40% RH brine solution. For FSW alone, scanning electrochemical cell microscopy and microelectrochemical syringe cell were utilized to understand the corrosion performance across the weld, in the retreating/advancing sides, and base material. Based on the results of this study, the FSW and cold spray repair techniques proved most viable for SCC repair in SS304 dry cask storage applications and continuing research is highly recommended to understand and quantify in further detail their SCC performance compared to unrepaired SS304. Additionally, solder and VFAW (patch or incline) would not be recommended based on the corrosion and SCC findings in this study.

42 ENGINEERING↗

Solid state welding of medium-entropy CrCoNi with heterogeneous, partially recrystallized microstructures

We report that heterogeneous, partially recrystallized (PRX) microstructures have recently been used to improve strength-ductility combinations in high-entropy alloys. However, these microstructures are incompatible with conventional joining processes that require melting or prolonged exposure to elevated temperatures. This work presents an initial exploration of solid state joining in this challenging condition using vaporizing foil actuator welding (VFAW) applied to PRX equiatomic alloy CrCoNi.

36 MATERIALS SCIENCE↗

Multi-scale characterization and simulation of impact welding between immiscible Mg/steel alloys

Vaporizing foil actuator spot welding method is used in this paper to join magnesium alloy AZ31 and uncoated high-strength steel DP590, which are typically considered as un-weldable due to their high physical property disparities, low mutual solubility, and the lack of any intermetallic phases. Characterization results from scanning electron microscopy (SEM) and high-resolution transmission electron microscopy (HRTEM) of the weld interface indicate that the impact creates an Mg nanocrystalline interlayer with abundant Fe particles. The interlayer exhibits intact bonding with both DP590 and AZ31 substrates. To investigate the fundamental bond formation mechanisms at the interface, a finite element (FE)-based process simulation is first performed to calculate the local temperature and deformation at the interface under the given macroscopic experimental condition. Finally, taking the FE results at the interface as inputs, molecular dynamics (MD) simulations are conducted to study the interlayer formation at the Mg/Fe interface during the impact and cooling. The results found a high velocity shearing-induced mechanical mixing mechanism that mixes Mg/Fe atoms at the interface and creates the interlayer, leading to the metallurgical bond between Mg/steel alloys.

36 MATERIALS SCIENCE↗

Cascading microstructures in aluminum-steel interfaces created by impact welding

With the rising need to develop light weight structures joining dissimilar metals is inevitable. Thus a fundamental understanding of the microstructure evolution and bond formation mechanism is necessary. In this work we probe the welded interface in aluminum and steel joined using vaporizing foil actuator welding (VFAW) a novel impact welding process. The goal of such a detailed characterization campaign is to understand the bond formation mechanism. The study demonstrates that the interfacial microstructure has a pronounced hierarchical nature. At the macro scale, the interface is characterized by a wavy interface which is a result of extensive plastic deformation that accompanies the process. Detailed transmission electron microscopy shows evidence for the formation of a liquid film at the interface resulting in significant inter diffusion of Fe. The solidified structure at the interface consisted of crystalline α-Al and an amorphous metastable Al-Fe intermetallic compound similar to the observations in rapid solidification of Al-Fe alloys. The sub-nm scale characterization of the interface using atom probe tomography showed two distinct zones 1. A magnesium (5 at.%) and oxygen (15 at.%) rich (not detectable using energy dispersive spectroscopy) which was probably from the decomposition of the surface oxide film 2. The rapidly solidified reaction zone consisting of primary crystalline α-Al and an amorphous Al-Fe (15 at.%)-O (0.5 at.%)-Si (1.5 at.%).Based on these observations a mechanism for the bond formation is presented.

36 MATERIALS SCIENCE↗

A robust process-structure model for predicting the joint interface structure in impact welding

The impact welding is gaining popularity in joining of dissimilar metals as any intermetallics are often very thin or discontinous with little to no heat affected zone resulting from the process. This work focuses on a recently developed impact welding technique, known as the Vaporizing Foil Actuator Welding (VFAW), which uses the pressure created from the electrically driven rapid vaporization of a thin metallic conductor to drive the flyer. A typical characteristic of an impact-welded joint is the wavy weld interface which is attributed to the complex interfacial kinematics resulting from the high-speed oblique impact of the metal plates. A numerical simulation framework based on the finite element method (FEM) with Eulerian formalism is developed to model the high-speed impact between the metal plates. The model accounts for the thermomechanical interactions in the process and captures the complex interfacial deformations. A thorough validation of the model is achieved by comparing the wave characteristics obtained from numerical simulations with the experimental results from vaporizing foil actuator welding. The amplitude and wavelength of the interfacial waves and the resulting joint microstructure is shown to be strongly dependent on the process conditions and the specific material system, which is well captured by the model.

42 ENGINEERING↗

On Process, Structure, Property Relationships in Impact Welding of Aluminum 6061 and Steel 4130

Vaporizing Foil Actuator Welding process was used to weld 1mm thick aluminum alloy 6061 sheet to 3.2 mm thick 4130 grade steel plate. Temporal evolution of the flyer sheet velocity was recorded at four locations on the flyer sheet using photonic Doppler velocimetry. The welded samples were subjected to mechanical and microstructural characterization. Although the welded interface did not show a very wavy characteristic, the welds had substantial strength. Welds made with a softer temper, T4 alloy were found to be stronger than the one created with a harder, T6 temper alloy. A coupled Lagrangian-Eulerian numerical framework was also utilized to predict the structure of the interface based on the measured velocity profile. The model also depicted absence of large waves although the jetting phenomenon was observed, thereby providing insight into necessary conditions for impact welding.

Mao, Yu↗

Creep Behavior and Deformation Mechanisms for Nanocluster-Strengthened Ferritic Steels

Mechanically alloyed, nanostructured ferritic steels represent a class of alloys that can display high resistance to radiation and creep deformation, which are derived from the presence of nanoclusters, precipitates and solute segregation to the grain boundaries. The creep responses for a 14YWT nanostructured ferritic steel were measured over a range of temperatures and stress levels. The stress exponent was observed to vary non-linearly with applied stress; stress exponents were found to decrease with decreasing stress approaching unity at low stress. Transmission electron microscopy studies clearly demonstrated that creep deformation proceeds by a dislocation glide within nanoscale grains and that glide dislocations are attracted to and pinned by nanoclusters. In light of these observations, a new model of the creep response, inspired by the Kocks-Argon-Ashby model, is developed to explain the low creep rates and small stress exponents that are exhibited by these alloys.

36 MATERIALS SCIENCE↗

Effect of Gallium Focused Ion Beam Milling on Preparation of Aluminum Thin Foils

Focus Ion Beam (FIB) milling has greatly extended the utility of atom probe and TEM because it enables sample preparation with a level of dimensional control never before possible. Using FIB it is possible to extract the samples from desired and very specific locations. The artifacts associated with this sample preparation method must also be fully understood. In this work issues specifically relevant to the FIB milling of aluminum alloys are presented. After using the FIB as a sample preparation technique it is evident that gallium will concentrate in three areas of the sample: on the surface, on grain boundaries and at interphase boundaries. This work also shows that low energy Ar ion nanomilling is potentially quite effective for removing gallium implantation layers and gallium from the internal surfaces of aluminum thin foils.

36 MATERIALS SCIENCE↗

A TEM Study of Creep Deformation Mechanisms in Allvac 718Plus

A preliminary study on the evolution of creep deformation substructure in Ni-base superalloy Allvac 718Plus has been performed. Specimens crept at 620 MPa and at temperatures ranging from 690-732 C were examined utilizing diffraction contrast TEM characterization techniques. Creep was interrupted at 1-2.5% strain in order to study the deformation substructure following a limited amount of deformation. The dominant deformation modes at each of the test temperatures were highly planar in nature and involved shearing of the matrix and precipitates on {111} glide planes. In addition, paired a/2<110> dislocations were evident which suggest an antiphase boundary shearing mechanism. Creep induced microtwinning was also observed at the highest creep temperature which was created by identical a/6<112> Shockley partial dislocations that shear the matrix and precipitates on consecutive close packed {111} glide planes.

36 MATERIALS SCIENCE↗

Microstructure Characterization of Magnetic-Pulse-Welded AA 6061-T6 by Electron Backscattered Diffraction

The grain boundary crystallographic misorientations of magnetic-pulse-welded (MPW) aluminum alloy (AA) 6061-T6 in linear and tubular configurations were examined using the electron backscattered diffraction (EBSD) technique. A refined structure of heavily deformed grains with higher grain boundary angles was observed in linear welds. Significant spalling was observed away from the joints, in the interior of tubular welds. The results show the complex interaction of shock waves with the materials during this impact welding process.