Engineering Papers⌕ Search

Engineering topics

Cui, Y

Publications and source records attributed to Cui, Y.

At least 73 records · Page 4

Internal electric-field-lines distribution in CdZnTe detectors measured using X-ray mapping

The ideal operation of CdZnTe devices entails having a uniformly distributed internal electric field. Such uniformity especially is critical for thick long-drift-length detectors, such as large-volume CPG and 3-D multi-pixel devices. Using a high-spatial resolution X-ray mapping technique, we investigated the distribution of the electric field in real devices. Our measurements demonstrate that in thin detectors, <5 mm, the electric field-lines tend to bend away from the side surfaces (i.e., a focusing effect). In thick detectors, >1 cm, with a large aspect ratio (thickness-to-width ratio), we observed two effects: the electric field lines bending away from or towards the side surfaces, which we called, respectively, the focusing field-line distribution and the defocusing field-line distribution. In addition to these large-scale variations, the field-line distributions were locally perturbed by the presence of extended defects and residual strains existing inside the crystals. We present our data clearly demonstrating the non-uniformity of the internal electric field.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Investigations of Cadmium Manganese Telluride Crystals for Room-Temperature Radiation Detection

Cadmium manganese telluride (CMT) has high potential as a material for room-temperature nuclear-radiation detectors. We investigated indium-doped CMT crystals taken from the stable growth region of the ingot, and compared its characteristics with that from the last-to-freeze region. We employed different techniques, including synchrotron white-beam X-ray topography (SWBXT), current-voltage (I-V) measurements, and low-temperature photoluminescence spectra, and we also assessed their responses as detectors to irradiation exposure. The crystal from the stable growth region proved superior to that from the last-to-freeze region; it is a single-grain crystal, free of twins, and displayed a resistivity higher by two orders-of-magnitude. The segregation of indium dopant in the ingot might be responsible for its better resistivity. Furthermore, we recorded a good response in the detector fabricated from the crystal taken from the stable growth region; its ({mu}{tau}){sub e} value was 2.6 x 10{sup -3} cm{sup 2}/V, which is acceptable for thin detectors, including for applications in medicine.

98 NUCLEAR DISARMAMENT, SAFEGUARDS, AND PHYSICAL P↗

Electric Field Distribution of Cadmium Zinc Telluride (CZT)

Cadmium Zinc Telluride (CZT) is attracting increasing interest with its promise as a room-temperature nuclear-radiation-detector material. The distribution of the electric field in CZT detectors substantially affects their detection performance. At Brookhaven National Laboratory (BNL), we employed a synchrotron X-Ray mapping technique and a Pockels-effect measurement system to investigate this distribution in different detectors. Here, we report our latest experimental results with three detectors of different width/height ratios. A decrease in this ratio aggravates the non-uniform distribution of electric field, and focuses it on the central volume. Raising the bias voltage effectively can minimize such non-uniformity of the electric field distribution. The position of the maximum electric field is independent of the bias voltage; the difference between its maximum- and minimum-intensity of electric field increases with the applied bias voltage.

43 PARTICLE ACCELERATORS↗

Tapping mode microwave impedance microscopy

We report tapping mode microwave impedance imaging based on atomic force microscope platforms. The shielded cantilever probe is critical to localize the tip-sample interaction near the tip apex. The modulated tip-sample impedance can be accurately simulated by the finite-element analysis and the result agrees quantitatively to the experimental data on a series of thin-film dielectric samples. The tapping mode microwave imaging is also superior to the contact mode in that the thermal drift in a long time scale is totally eliminated and an absolute measurement on the dielectric properties is possible. We demonstrated tapping images on working nanodevices, and the data are consistent with the transport results.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Opto-electrical characterization and X-ray mapping of large-volume cadmium zinc telluride radiation detectors

Large-volume cadmium zinc telluride (CZT) radiation detectors would greatly improve radiation detection capabilities and, therefore, attract extensive scientific and commercial interests. CZT crystals with volumes as large as hundreds of centimeters can be achieved today due to improvements in the crystal growth technology. However, the poor performance of large-volume CZT detectors is still a challenging problem affecting the commercialization of CZT detectors and imaging arrays. We have employed Pockels effect measurements and synchrotron X-ray mapping techniques to investigate the performance-limiting factors for large-volume CZT detectors. Experimental results with the above characterization methods reveal the non-uniform distribution of internal electric field of large-volume CZT detectors, which help us to better understand the responsible mechanism for the insufficient carrier collection in large-volume CZT detectors.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

CZT Virtual Frisch-grid Detector: Principles and Applications

Cadmium Zinc Telluride (CdZnTe or CZT) is a very attractive material for using as room-temperature semiconductor detectors, because it has a wide bandgap and a high atomic number. However, due to the material's poor hole mobility, several special techniques were developed to ensure its suitability for radiation detection. Among them, the virtual Frisch-grid CZT detector is an attractive option, having a simple configuration, yet delivering an outstanding spectral performance. The goal of our group in Brookhaven National Laboratory (BNL) is to improve the performance of Frisch-ring CZT detectors; most recently, that effort focused on the non-contacting Frisch-ring detector, allowing us to build an inexpensive, large-volume detector array with high energy-resolution and a large effective area. In this paper, the principles of virtual Frisch-grid detectors are described, especially BNL's innovative improvements. The potential applications of virtual Frisch-grid detectors are discussed, and as an example, a hand-held gamma-ray spectrometer using a CZT virtual Frischgrid detector array is introduced, which is a self-contained device with a radiation detector, readout circuit, communication circuit, and high-voltage supply. It has good energy resolution of 1.4% (FWHM of 662-keV peak) with a total detection volume of {approx}20 cm{sup 3}. Such a portable inexpensive device can be used widely in nonproliferation applications, non-destructive detection, radiation imaging, and for homeland security. Extended systems based on the same technology have potential applications in industrial- and nuclear-medical-imaging.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Material properties limiting the performance of CZT gamma-ray detectors

CdZnTe (CZT) nuclear radiation detectors are advanced sensors that utilize innovative technologies developed for wide band-gap semiconductor industry and microelectronics. They open opportunities for new types of room-temperature operating, field deployable instruments that provide accurate identification of potential radiological threats and timely awareness for both the civilian and military communities. Room-temperature radiation detectors are an emerging technology that relies on the use of high-quality CZT crystals whose availability is currently limited by material non-uniformities and the presence of extended defects. To address these issues, which are most critical to CZT sensor developments, we developed X-ray mapping and IR transmission microscopy systems to characterize both CZT crystals and devices. Since a customized system is required for such X-ray measurements, we use synchrotron radiation beams available at BNL's National Synchrotron Light Source. A highly-collimated and high-intensity X-ray beam supports measurements of areas as small as 10 x 10 {micro}m{sup 2}, and allowed us to see fluctuations in collected charge over the entire area of the detector in a reasonable time. The IR microscopy system allows for 3D visualization of Te inclusions and other extended defects. In this paper, we describe the experimental techniques used in our measurements and typical results obtained from CZT samples produced by different suppliers.

43 PARTICLE ACCELERATORS↗

Internal Electric Field Investigations of a Cadmium Zinc Telluride Detector Using Synchrotron X-ray Mapping and Pockels Effect Measurements

Cadmium zinc telluride (CZT) has remained a major focus of research due to its promising application as a room-temperature nuclear radiation detector material. Among the several parameters that substantially affect the detectors' performance, an important one is the distribution of the internal electric field. Brookhaven National Laboratory (BNL) employed synchrotron x-ray microscale mapping and measurements of the Pockels effect to investigate the distribution of the internal electric field in a CZT strip detector. Direct evidence that dislocations can distort the internal electric field of the detector was obtained. Furthermore, it was found that 'star' defects in the CZT crystal, possibly ascribed to dislocation loop punching, cause charge trapping.

43 PARTICLE ACCELERATORS↗

Optical Absorption Enhancement in Amorphous Silicon Nanowire and Nanocone Arrays

Hydrogenated amorphous Si (a-Si:H) is an important solar cell material. Here we demonstrate the fabrication of a-Si:H nanowires (NWs) and nanocones (NCs), using an easily scalable and IC-compatible process. We also investigate the optical properties of these nanostructures. These a-Si:H nanostructures display greatly enhanced absorption over a large range of wavelengths and angles of incidence, due to suppressed reflection. The enhancement effect is particularly strong for a-Si:H NC arrays, which provide nearly perfect impedance matching between a-Si:H and air through a gradual reduction of the effective refractive index. More than 90% of light is absorbed at angles of incidence up to 60{sup o} for a-Si:H NC arrays, which is significantly better than NW arrays (70%) and thin films (45%). In addition, the absorption of NC arrays is 88% at the band gap edge of a-Si:H, which is much higher than NW arrays (70%) and thin films (53%). Our experimental data agree very well with simulation. The a-Si:H nanocones function as both absorber and antireflection layers, which offer a promising approach to enhance the solar cell energy conversion efficiency.

14 SOLAR ENERGY↗

Internal Electric-Field-Lines Distribution in Cdznte Detectors Measured Using X-ray Mapping

The ideal operation of CdZnTe devices entails having a uniformly distributed internal electric field. Such uniformity especially is critical for thick long-drift-length detectors, such as large-volume CPG and 3-D multi-pixel devices. Using a high-spatial resolution X-ray mapping technique, we investigated the distribution of the electric field in real devices. Our measurements demonstrate that in thin detectors, < 5 mm, the electric field-lines tend to bend away from the side surfaces (i.e., a focusing effect). In thick detectors, > 1 cm, with a large aspect ratio (thickness-to-width ratio), we observed two effects: the electric field lines bending away from or towards the side surfaces, which we called, respectively, the focusing field-line distribution and the defocusing field-line distribution. In addition to these large-scale variations, the field-line distributions were locally perturbed by the presence of extended defects and residual strains existing inside the crystals. We present our data clearly demonstrating the non-uniformity of the internal electric field.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Extended Defects in Cdznte Radiation Detectors

Large-volume CdZnTe (CZT) single crystals with electron lifetime exceeding 10 mus have recently become commercially available. This opened the opportunity for making room temperature CZT gamma-ray detectors with extended thicknesses and larger effective areas. However, the extended defects that are present even in the highest-quality material remain a major drawback which affects the availability and cost of large CZT detectors. In contrast to the point defects that control electron lifetime and whose effects on the charge collection can be electronically corrected, the extended defects introduce significant fluctuations in the collected charge, which increase with a crystal's thickness. The extended defects limit the uniformity in the electrons' drift distance in CZT crystals, above which electron trapping cannot effectively be corrected. In this paper, we illustrate the roles of the extended defects in CZT detectors with different geometries. We emphasize that the crystallinity of commercial CZT materials remains a major obstacle on the path to developing thick, large-volume CZT detectors for gamma-ray imaging and spectroscopy.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Effect of Te Inclusions on the Performance of Cdznte Radiation Detectors

Te inclusions existing at high concentrations in CdZnTe (CZT) material can degrade the performance of CZT detectors. These microscopic defects trap the free electrons generated by incident radiation, so entailing significant fluctuations in the total collected charge and thereby strongly affecting the energy resolution of thick (long-drift) detectors. Such effects were demonstrated in thin planar detectors, and, in many cases, they proved to be the dominant cause of the low performance of thick detectors, wherein the fluctuations in the charge losses accumulate along the charge's drift path. We continued studying this effect using different tools and techniques. We employed a dedicated beamline recently established at BNL's National Synchrotron Light Source for characterizing semiconductor radiation detectors, along with an IR transmission microscope system, the combination of which allowed us to correlate the concentration of defects with the devices' performances. We present here our new results from testing over 50 CZT samples grown by different techniques. Our goals are to establish tolerable limits on the size and concentrations of these detrimental Te inclusions in CZT material, and to provide feedback to crystal growers to reduce their numbers in the material.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Impurity Gettering Effect of Te Inclusions in Cdznte Single Crystals

The local impurity distribution in Te inclusions of CdZnTe (CZT) crystal was investigated by the time-of-flight secondary ion mass spectrometry (Tof-SIMS) technique. Direct evidence of impurity gettering in Te inclusions has been observed for the first time. The impurity gettering in Te inclusions originated from the diffusion mechanism during crystal growth and segregation mechanism during crystal cooling. This phenomenon is meaningful, because it reveals how Te inclusions affect CZT properties and provides a possible approach to reduce the impurities in CZT by the way of removing Te inclusions.

36 MATERIALS SCIENCE↗

Surface Plasmon Excitation via Au Nanoparticles in CdSe Semiconductor

We present experimental evidence for the large Raman and photoluminescence enhancement in CdSe semiconductor films grown on Si and glass substrates due to excitation of surface plasmon resonances in proximate gold metal nanoparticles deposited on the surface of CdSe film. Heterojunction diodes containing n-CdSe on p-Si semiconductor were fabricated and the surface of the diodes was in situ coated with Au nanoparticles using the ultra-high vacuum pulsed-laser deposition technique. A significant enhancement of the photocurrent was obtained in CdSe/p-Si containing Au nanoparticles on the surface compared to CdSe/p-Si due to the enhanced photo-absorption within the semiconductor by the phenomenon of surface plasmon resonance. These observations suggest a variety of approaches for improving the performance of devices such as photodetectors, photovoltaic, and related devices, including biosensors.

36 MATERIALS SCIENCE↗

Investigation of Charge Transport Properties of CdZnTe Detectors with Synchrotron X-ray Radiation

Various internal defects, such as Te inclusions, twin boundaries, dislocation, etc., are prevalent in as-grown CdZnTe (CZT) crystals, which affect the charge transport properties of CZT crystals and, therefore, worsen the performance of CZT detectors. In order to develop high quality CZT detectors, it is imperative to clarify the effects of internal defects on the charge transport properties of CZT. Simple flood illumination with nuclear radiation source cannot reveal the nature of highly localized defects in CZT. Therefore, at Brookhaven's National Synchrotron Light Source (NSLS), we have developed a unique testing system for micro-scale defect investigation of CZT, which employs an X-ray beam collimated with the spatial resolution as small as 3 x 3 {micro}m{sup 2}, a microscopic size comparable to the scale of common defects in CZT. This powerful tool enables us to investigate the effect of internal defects on charge transport properties of CZT in detail.

43 PARTICLE ACCELERATORS↗

Good electrical contacts for high resistivity (Cd,Mn)Te crystals

We consider that semi-insulating (Cd,Mn)Te crystals may well successfully replace the commonly used (Cd,Zn)Te crystals as a material for manufacturing large-area X- and gamma-ray detectors. The Bridgman growth method yields good quality and high-resistivity (10{sup 9}-10{sup 10} {Omega}-cm) crystals of (Cd,Mn)Te:V. Doping with vanadium ({approx} 10{sup 16} cm{sup -3}), which acts as a compensating agent, and annealing in cadmium vapors, which reduces the number of cadmium vacancies in the as-grown crystal, ensure this high resistivity. Detector applications of the crystals require satisfactory electrical contacts. Hence, we explored techniques of ensuring good electrical contacts to semi-insulating (Cd,Mn)Te crystals. Our findings are reported here. Before depositing the contact layers, we prepared an 'epi-ready' surface of the crystal platelet by a procedure described earlier for various tellurium-based II-VI compound crystals. A molecular beam epitaxy (MBE) apparatus was used to deposit various types of contact layers: Monocrystalline semiconductor layers, amorphous- and nanocrystalline semiconductor layers, and metal layers were studied. We employed ZnTe heavily doped ({approx} 10{sup 18} cm{sup -3}) with Sb, and CdTe heavily doped ({approx} 10{sup 17} cm{sup -3}) with In as the semiconductors to create contact layers that subsequently enable good contact (with a narrow, tunneling barrier) to the Au layer that usually is applied as the top contact layer. We describe and discuss the technology and some properties of the electrical contacts to semi-insulating (Cd,Mn)Te.

36 MATERIALS SCIENCE↗

(Cd,Mn)Te detectors for characterization of x-ray emissions generated during laser-driven fusion experiments

We present our measurements of (Cd,Mn)Te photoconductive detectors (PCDs), fabricated for the goal of measuring both the temporal and spectral dependences of X-ray emissions generated from laser-illuminated targets during the inertial confinement fusion experiments. Our Cd{sub 1-x}Mn{sub x}Te (x = 0.05) single crystals, doped with V, were grown using a vertical Bridgman method and, subsequently, annealed in Cd for the highest resistivity ({approx}10{sup 10} {Omega}cm) and a good mobility-lifetime product ({approx}10{sup -3} cm{sup 2}/V). The 1-mm- and 2.3-mm-thick detectors were placed in the same housing as two 1-mm-thick diamond PCDs. All devices were pre-screened by a 7.6-mm-thick Be X-ray filter with a frequency cutoff of 1 keV. The incident shots from the OMEGA laser were 1-ns-long square pulses with energies ranging from 2.3 kJ to 22.6 kJ, and the PCDs were biased with 5000 V/cm. The response amplitudes and rise times of our (Cd,Mn)Te PCDs were comparable with the diamond detector performance, while the decay times were 4 to 10 times longer and in the 2-5 ns range. We observed two X-ray emission events separated by 1.24 ns. The first was identified as caused by heating of the target and creating a hot corona, while the second one was from the resulting compressed core. For comparison purposes, our testing was performed using {approx}1 keV X-ray photons, optimal for the diamond PCD. According to the presented simulations, however, at X-ray energies >10 keV diamond absorption efficiency drops to <50%, whereas for (Cd,Mn)Te the drop occurs at {approx}100 keV with near perfect, 100% absorption, up to 50 keV.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗