Engineering Papers⌕ Search

Engineering topics

Chen, Xiang

Publications and source records attributed to Chen, Xiang.

134 records · Page 8

Application of Direct Current Potential Drop for the J-integral vs. Crack Growth Resistance Curve Characterization

The direct current potential drop (DCPD) technique has been applied to derive the J-integral vs. crack growth resistance curve (J-R curve) for fracture toughness characterization of structural materials. The test matrix covered three materials including type 316LN stainless steels, Ni-based alloy 617, and one ferritic-martensitic steel, three specimen configurations including standard compact, single edge bending, and disk-shaped compact specimens, and temperatures ranging from 20 C to 650 C. When compared with baseline J-R curves derived from the ASTM normalization method, the original J-R curves from the DCPD technique yielded much smaller Jq values due to the influence of crack blunting, plastic deformation, etc. on potential drop. To counter these effects, a new procedure for adjusting DCPD J-R curves was proposed. After applying the new adjustment procedure, the average difference in Jq between the DCPD technique and the normalization method was only 5.2% and the difference in tearing modulus was 7.4%. The promising result demonstrates the applicability of the DCPD technique for the J-R curve characterization especially in extreme environments, such as elevated temperatures, where the conventional elastic unloading compliance method faces considerable challenges.

DCPD↗

J-R Curve Determination for Disk-shaped Compact Specimens Based on the Normalization Method and Direct Current Potential Drop Technique

Material ductile fracture toughness can be described by J-integral versus crack extension relationship (J-R curve). As a conventional J-R curve measurement method, unloading compliance (UC) becomes impractical in elevated temperature testing due to relaxation of the material and a friction induced back-up shape of the J-R curve. In addition, the UC method may underpredict the crack extension for standard disk-shaped compact (DC(T)) specimens. In order to address these issues, the normalization method and direct current potential drop (DCPD) technique were applied for determining J-R curves at 24 C and 500 C for 0.18T DC(T) specimens made from type 316L stainless steel. For comparison purchase, the UC method was also applied in 24 C tests. The normalization method was able to yield valid J-R curves in all tests. The J-R curves from the DCPD technique need adjustment to account for the potential drop induced by plastic deformation, crack blunting, etc. and after applying a newly-developed DCPD adjustment procedure, the post-adjusted DCPD J-R curves essentially matched J-R curves from the normalization method. In contrast, the UC method underpredicted the crack extension in all tests resulting in substantial deviation in the derived J-R curves manifested by high Jq values than the normalization or DCPD method. Only for tests where the UC method underpredicted the crack extension by a very small value, J-R curves determined by the UC method were similar to those determined by the normalization or DCPD method.

DCPD↗

Experimental and modeling results of creep fatigue life of Inconel 617 and Haynes 230 at 850 C

Creep fatigue testing of Ni-based superalloy Inconel 617 and Haynes 230 were conducted in the air at 850 C. Tests were performed with fully reversed axial strain control at a total strain range of 0.5%, 1.0% or 1.5% and hold time at maximum tensile strain for 3, 10 or 30 min. In addition, two creep fatigue life prediction methods, i.e. linear damage summation and frequency-modified tensile hysteresis energy modeling, were evaluated and compared with experimental results. Under all creep fatigue tests, Haynes 230 performed better than Inconel 617. Compared to the low cycle fatigue life, the cycles to failure for both materials decreased under creep fatigue test conditions. Longer hold time at maximum tensile strain would cause a further reduction in both material creep fatigue life. The linear damage summation could predict the creep fatigue life of Inconel 617 for limited test conditions, but considerably underestimated the creep fatigue life of Haynes 230. In contrast, frequency-modified tensile hysteresis energy modeling showed promising creep fatigue life prediction results for both materials.

Chen, Xiang↗

Low cycle fatigue and creep-fatigue behavior of Ni-based alloy 230 at 850 C

Strain-controlled low cycle fatigue (LCF) and creep-fatigue testing of Ni-based alloy 230 were carried out at 850 C. The material creep-fatigue life decreased compared with its low cycle fatigue life at the same total strain range. Longer hold time at peak tensile strain further reduced the material creep-fatigue life. Based on the electron backscatter diffraction, a novel material deformation characterization method was applied, which revealed that in low cycle fatigue testing as the total strain range increased, the deformation was segregated to grain boundaries since the test temperature was higher than the material equicohesive temperature and grain boundaries became weaker regions compared with grains. Creep-fatigue tests enhanced the localized deformation, resulting in material interior intergranular cracking, and accelerated material damage. Precipitation in alloy 230 helped slip dispersion, favorable for fatigue property, but grain boundary cellular precipitates formed after material exposure to the elevated temperature had a deleterious effect on the material low cycle fatigue and creep-fatigue property.

Creep-fatigue↗

Application of Direct Current Potential Drop for Fracture Toughness Measurement

Material fracture toughness based on J-integral versus crack-extension relationship (J-R curve) is investigated with direct current potential drop (DCPD) technique and compared with results from elastic unloading compliance (EUC) or normalization technique. The test matrix covered four different materials, half inch thickness and one inch thickness compact tension (C(T))specimens, and temperatures ranging from 24 C to 600 C. The original J-R curves from DCPD yielded much smaller Jq value than EUC or normalization results due to the influence of plastic deformation on potential drop. To counter this effect, two new methods for adjusting DCPD data have been proposed. After adjustment, the average difference in Jq between DCPD and EUC or normalization results is only about 8% whereas the difference in tearing modulus is about 17%. The promising results prove the applicability of DCPD for J-R curve determination for C(T) specimens especially in extreme environments, such as elevated temperatures, where conventional EUC method faces considerable challenges.

Chen, Xiang↗

FRACTURE TOUGHNESS OF 9Cr-1MoV AND THERMALLY AGED ALLOY 617 FOR ADVANCED REACTOR APPLICATIONS

Nickel-base Alloy 617 is being considered as a structural material for application in the secondary heat exchanger of the New Generation Nuclear Plant, a very high temperature gas-cooled reactor. Thermal aging of Alloy 617 plate and welds is being performed with tensile, Charpy impact, and fracture toughness tests conducted at temperatures to 950 C. Results of testing for thermal aging to 5,300 h have been obtained and are presented; varying effects of thermal aging temperature and time on fracture toughness are observed. The 9Cr-1MoV (Grade 91) ferritic steel is a candidate for structural applications in the sodium fast reactor. Fracture toughness testing of unaged Grade 91 steel has been performed to evaluate specimen size effects in preparation for future testing of the material in the thermally aged condition. Results for material in the mill-annealed and heat treated conditions are presented and show that this heat of Grade 91 steel does not indicate a small specimen bias on the fracture toughness Master Curve reference temperature.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Gear optimization

The use of formal numerical optimization methods for the design of gears is investigated. To achieve this, computer codes were developed for the analysis of spur gears and spiral bevel gears. These codes calculate the life, dynamic load, bending strength, surface durability, gear weight and size, and various geometric parameters. It is necessary to calculate all such important responses because they all represent competing requirements in the design process. The codes developed here were written in subroutine form and coupled to the COPES/ADS general purpose optimization program. This code allows the user to define the optimization problem at the time of program execution. Typical design variables include face width, number of teeth and diametral pitch. The user is free to choose any calculated response as the design objective to minimize or maximize and may impose lower and upper bounds on any calculated responses. Typical examples include life maximization with limits on dynamic load, stress, weight, etc. or minimization of weight subject to limits on life, dynamic load, etc. The research codes were written in modular form for easy expansion and so that they could be combined to create a multiple reduction optimization capability in future.

Vanderplaats, G. N.↗