Mesoscale Phase Distribution in Single Particles of LiFePO 4 following Lithium Deintercalation
Explore the source record for details and available documents.
Engineering topics
Publications and source records attributed to Chen, Guoying.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Overcharge protection for 4 V Li{sub 1.05}Mn{sub 1.95}O{sub 4}/lithium cells at charging rates in excess of 1 mA/cm{sup 2} (3C) and at temperatures as low as -20 C was achieved using a bilayer separator coated with two electroactive polymers. High rate and low temperature overcharge protection and discharge performance were improved by employing a design in which the polymer-coated portion of the separator is in parallel with the cell rather than between the electrodes. The effects of different membrane supports for the electroactive polymers are also examined.
It is shown that the rate performance of a lithium battery composite electrode may be compromised by poor internal connectivity due to defects and inhomogeneities introduced during electrode fabrication or subsequent handling. Application of a thin conductive coating to the top surface of the electrode or to the separator surface in contact with the electrode improves the performance by providing alternative current paths to partially isolated particles of electroactive material. Mechanistic implications are discussed and strategies for improvement in electrode design and fabrication are presented.
Li and 3IP NMR experiments were conducted on a series of single- or two-phase samples in the LiFePCvFePCM system with different overall lithium contents, and containing the two end-members and/or two metastable solid solution hases, Lio.6FeP04 or Lio.34FeP04. These experiments were carried out at different temperatures in order to search for vacancy/charge ordering and ion/electron mobility in the metastable phases. Evidence for Li+-Fe2+ interactions was bserved for both Lio.6FeP04 and Lio.34FePC>4. The strength of this interaction leads to the formation of LiFePCvlike clusters in the latter, as shown by the room temperature data. Different motional processes are proposed to exist as the temperature is increased and various scenarios are discussed. While concerted lithium-electron hopping and/or correlations explains the data below 125C, evidence for some uncorrelated motion is found at higher temperatures, together with the onset of phase mixing.
The remarkable thermal stability of LiFePO{sub 4} and its charged counterpart, FePO{sub 4}, have been instrumental in its commercialization as a lithium ion battery cathode material. Despite the similarity in composition and structure, and despite the high thermal stability of the parent compound, LiMnPO{sub 4}, we find that the delithiated phase Li{sub y}MnPO{sub 4}, (which contains a small amount of residual lithium), is relatively unstable and reactive toward a lithium ion electrolyte. The onset temperature for heat evolution in the presence of 1M LiPF{sub 6} in 1:1 ethylene carbonate/propylene carbonate is around 150 C, and the total evolved heat is 884 J/g, comparable to that produced under similar conditions by charged LiCoO{sub 2} electrodes.
Nonstoichiometry is reported in the LiMnPO{sub 4}/MnPO{sub 4} system for the first time. As lithium is removed from crystalline LiMnPO{sub 4} by chemical or electrochemical methods, the resulting two phase mixture consists of stoichiometric LiMnPO{sub 4} and a delithiated phase, Li{sub y}MnPO{sub 4}, whose lattice parameters depend upon the global extent of delithiation and on the crystalline domain size of the delithiated phase. This behavior is reproduced during electrochemical insertion of lithium. Again, no evidence for nonstoichiometry was found in the vicinity of LiMnPO{sub 4}. Attempts to create single phase solid solutions by heating mixtures of the two phases failed due to the thermal instability of Li{sub y}MnPO{sub 4}.
Highly crystalline samples of LiMnPO{sub 4} and its analogs with partial substitution of Mn by divalent Mg, Cu, Zn, and Ni were prepared by hydrothermal synthesis and characterized by x-ray diffraction and infrared spectroscopy. Chemical oxidation produced two-phase mixtures of the initial phases LiMn{sub (1-y)}M{sub y}PO{sub 4} and the delithiated forms, Li{sub y}Mn{sub (1-y)}M{sub y}PO{sub 4}, all with the olivine structure. The extent of oxidation depended upon the quantity of oxidizing agent used and on the identity of the substituent ions. Mg, Ni and Cu were found to increase the level of delithation relative to that in pure LiMnPO{sub 4}. Mg was also shown to reduce the tendency of the oxidized phase to absorb water.