Engineering Papers⌕ Search

Engineering topics

Ban, Chunmei

Publications and source records attributed to Ban, Chunmei.

At least 37 records · Page 2

Fast Determination of Lithium Content in Spent Cathodes for Direct Battery Recycling

Determination of the lithium ion content in cathode materials, which is currently performed by inductively coupled plasma mass spectrometry (ICP-MS), involves tedious procedures and error-prone preparation. This work introduces a new methodology to quickly determine the lithium content in spent cathode materials (LiNix Mny Coz O2, x + y + z = 1, NMC) using a thermalgravimetric analysis, which bypasses the use of ICP-MS and significantly reduces the cost and time required for determining the lithium content. Based on this new method, a new approach is developed to identify spent cathode materials suitable for direct relithiation recycling. Finally, these new methods have been applied to investigate the effectiveness of direct electrochemical-relithiation on recycling the spent cathodes, and provide insights for future development of direct battery materials recycling.

cathode recycling↗

Nonpassivated Silicon Anode Surface

A stable solid electrolyte interphase (SEI) has been proven to be a key enabler to most advanced battery chemistries, where the reactivity between the electrolyte and the anode operating beyond the electrolyte stability limits must be kinetically suppressed by such SEIs. The graphite anode used in state-of-the-art Li-ion batteries presents the most representative SEI example. Because of similar operation potentials between graphite and silicon (Si), a similar passivation mechanism has been thought to apply on the Si anode when using the same carbonate-based electrolytes. Herein, we found that the chemical formation process of a proto-SEI on Si is closely entangled with incessant SEI decomposition, detachment, and reparation, which lead to continuous lithium consumption. Using a special galvanostatic protocol designed to observe the SEI formation prior to Si lithiation, we were able to deconvolute the electrochemical formation of such dynamic SEI from the morphology and mechanical complexities of Si and showed that a pristine Si anode could not be fully passivated in carbonate-based electrolytes.

25 ENERGY STORAGE↗

Surface SiO 2 Thickness Controls Uniform-to-Localized Transition in Lithiation of Silicon Anodes for Lithium-Ion Batteries

Silicon is a promising anode material for lithium-ion batteries because of its high capacity, but its widespread adoption has been hampered by a low cycle life arising from mechanical failure and the absence of a stable solid–electrolyte interphase (SEI). Understanding SEI formation and its impact on cycle life is made more complex by the oxidation of silicon materials in air or during synthesis, which leads to SiO x coatings of varying thicknesses that form the true surface of the electrode. Here, the lithiation of SiO 2 -coated Si is studied in a controlled manner using SiO 2 coatings of different thicknesses grown on Si wafers via thermal oxidation. SiO 2 thickness has a profound effect on lithiation: below 2 nm, SEI formation followed by uniform lithiation occurs at positive voltages versus Li/Li + . Si lithiation is reversible, and SiO 2 lithiation is largely irreversible. Above 2 nm SiO 2 , voltammetric currents decrease exponentially with SiO 2 thickness. For 2–3 nm SiO 2 , SEI formation above 0.1 V is suppressed, but a hold at low or negative voltages can initiate charge transfer whereupon SEI formation and uniform lithiation occur. Cycling of Si anodes with an SiO 2 coating thinner than 3 nm occurs at high Coulombic efficiency (CE). If an SiO 2 coating is thicker than 3–4 nm, the behavior is totally different: lithiation at positive voltages is strongly inhibited, and lithiation occurs at poor CE and is highly localized at pinholes which grow over time. As they grow, lithiation becomes more facile and the CE increases. Pinhole growth is proposed to occur via rapid transport of Li along the SiO 2 /Si interface radially outward from an existing pinhole, followed by the lithiation of SiO 2 from the interface outward.

25 ENERGY STORAGE↗

Improved Stability and Cyclability of Ceramic Solid Electrolyte by Coating Polymer

Rechargeable all-solid-state lithium (Li) metal batteries show better safety and energy density compared to commercial Li-ion batteries using liquid electrolyte. As the key component of Li metal batteries, ceramic solid-state electrolyte has attracted great interest because of its high ion conductivity and great potential in interfacing with Li metal. Ceramic electrolyte has a more stable interface with Li metal than liquid electrolyte, but chemical reaction and Li dendrite growth at the electrolyte/Li interface are still significant, which causes device degradation and failure by cycling of Li plating and stripping. Unlike ceramic electrolyte, polymer electrolyte has a relatively stable interface with Li metal and better mechanical flexibility. Therefore, we introduced a polymer electrolyte coating to protect the ceramic electrolyte from direct contact with Li metal. The galvanotactic cycling Li plating/striping data on the devices with (without) the coating illustrates increased (decreased) overall conductivity and cyclability of the test cell by the cycling. Nanometer-scale ionic-transport imaging, based on atomic force microscopy, shows that cycling degrades the ceramic-only electrolyte by partially blocking ionic transport in areas; in contrast, cycling on the polymer-coated electrolyte improves ionic conductivity. Compared with the ceramic-only electrolyte, this novel polymer electrolyte coating on ceramic electrolyte shows less degradation when in contact with Li metal.

25 ENERGY STORAGE↗

Magnesium-based methods, systems, and devices

An aspect of the present invention is an electrical device, where the device includes a current collector and a porous active layer electrically connected to the current collector to form an electrode. The porous active layer includes MgBx particles, where x≥1, mixed with a conductive additive and a binder additive to form empty interstitial spaces between the MgBx particles, the conductive additive, and the binder additive. The MgBx particles include a plurality of boron sheets of boron atoms covalently bound together, with a plurality of magnesium atoms reversibly intercalated between the boron sheets and ionically bound to the boron atoms.

36 MATERIALS SCIENCE↗

Three-Dimensional Resistivity vs. Depth Profiling for Advanced Characterization of the Lithium-Ion Battery Solid Electrolyte Interphase

In this work, we investigate the evolution of SEI formed from a standard electrolyte (1.2 M LiPF6 in EC:EMC (3:7 wt%)) through various points in cycling on several model Si surfaces. We also examine the solubility of SEI by resting the anode in the cell at varied temperatures then characterizing the residual SEI. Evolution of the SEI surface is also analyzed with atomic force microscopy (AFM) measurements. AFM and SSRM-derived results are presented in combination with chemical characterization, including time-of-flight secondary ion mass spectrometry (TOF-SIMS).

25 ENERGY STORAGE↗

Temperature-Dependent Solubility of Solid Electrolyte Interphase on Silicon Electrodes

The lithium-ion batteries powering mass market electric vehicles must be capable of operating in a wide temperature range. Temperature variation has the possibility to greatly affect the stability of the solid electrolyte interphase (SEI) responsible for mitigating capacity fade due to electrolyte decomposition in the lithium-ion battery. Here, we explore the solubility of the SEI on the silicon (Si) electrode, an alternative anode material to the conventional graphite electrode, at temperatures ranging from -10 to 50 °C. Through use of an electrochemical protocol with a high cathodic cutoff voltage, we measure the evolution of the SEI independently of competing Si mechanical stress. We correlate the electrochemical data with three-dimensional resistivity versus depth profiling as well as atomic force microscopy to show that SEI dissolution occurs at significantly faster rates at higher temperatures.

25 ENERGY STORAGE↗

Microstructure Study on Initial Lithiation/Delithiation Cycle of Crystalline Silicon Wafer

In this work, we found that Si wafer has a preferential expansion along <110> directions during the initial lithiation/delithiation cycle, as the evidence of wider <110> cracks. These cracks also propagate much deep, at least 5 um. The morphology of the amorphous Si layer appearing after the initial cycle shows a dependence on the plane orientation, i.e., multi and deep layers on the {110} plane, where as a single layer with ~200nm on the {100} plane.A PAA coating layer on the Si wafer mitigates the cracks and reduces the thickness of the amorphous Si layer.

14 SOLAR ENERGY↗

Materials for flow battery energy storage and methods of using

The present disclosure relates to a mixture that includes a mediator having a first redox potential, a non-liquid active material having a second redox potential that is less than the first redox potential, and a cation. In addition, the non-liquid active material has a first condition that includes a first oxidation state, where the cation is intercalated within the non-liquid active material, and the non-liquid active material has a second condition that includes a second oxidation state that is higher than the first oxidation state, where the non-liquid active material is substantially free of the cation. In addition, the mediator has a first condition that includes a third oxidation state and a second condition that includes a fourth oxidation state that is higher than the third oxidation state. In addition, the non-liquid active material is capable of being reversibly cycled between its first condition and its second condition, and the mediator is capable of being reversibly cycled between its first condition and its second condition.

25 ENERGY STORAGE↗

Atomic layer deposition in porous electrodes: A pore-scale modeling study

Coating porous electrodes of Li-ion batteries with functional materials by atomic layer deposition (ALD) can enhance their capacity stability. Because of the complex microstructure of the porous electrodes, predicting the required exposure time of the precursors for achieving a desired coating and the coating characteristics for a given exposure time remains difficult. Here, a three-dimensional (3D) pore-scale lattice Boltzmann model is developed to investigate the reactive transport processes during the ALD of reconstructed electrodes and to assess the accuracy of one-dimensional (1D) mean-field models. The effects of the hierarchical structure of pores and their connectivity on the coating process of ALD are investigated and the detailed coating characteristics in the electrodes are resolved. Electrodes with smaller pore sizes requires a longer exposure time to achieve full coating. At the same depth within an electrode, the smaller pores are coated more slowly than the wider pores (especially at high Damkohler numbers) and the coating speed of well-connected pores are faster than that of poorly connected pores. Furthermore, simulations also reveal that the 1D mean-field model can capture the average coating characteristics reasonably well when pores in the electrodes are well connected but may perform poorly if the pores are poorly connected.

25 ENERGY STORAGE↗

Spatially Resolving Lithiation in Silicon–Graphite Composite Electrodes via in Situ High-Energy X-ray Diffraction Computed Tomography

Optimizing the chemical and morphological parameters of lithium-ion (Li-ion) electrodes is extremely challenging, due in part to the absence of techniques to construct spatial and temporal descriptions of chemical and morphological heterogeneities. We present the first demonstration of combined high-speed X-ray diffraction (XRD) and XRD computed tomography (XRD-CT) to probe, in 3D, crystallographic heterogeneities within Li-ion electrodes with a spatial resolution of 1 um. The local charge-transfer mechanism within and between individual particles was investigated in a silicon(Si)-graphite composite electrode. Here, high-speed XRD revealed charge balancing kinetics between the graphite and Si during the minutes following the transition from operation to open circuit. Subparticle lithiation heterogeneities in both Si and graphite were observed using XRD-CT, where the core and shell structures were segmented, and their respective diffraction patterns were characterized.

36 MATERIALS SCIENCE↗

Spatial Molecular Layer Deposition of Ultrathin Polyamide To Stabilize Silicon Anodes in Lithium-Ion Batteries

Cycling stability is central to implementing silicon (Si) anodes in next-generation high-energy lithium-ion batteries. However, challenges remain due to the lack of effective strategies to enhance the structural integrity of the anode during electrochemical cycling. Here, we develop a nanoscale polyamide coating, using spatial molecular layer deposition (MLD) of m-phenylenediamine and trimesoyl chloride precursors, to preserve the structural integrity of Si anodes. Poly(acrylic acid) (PAA) has been widely used in Si-based anodes as a binding agent due to its effective binding interactions with Si particles. However, the structural integrity of the anode is compromised by thermochemical decomposition of the poly(acrylic acid) binder, which can occur during electrode drying or during electrochemical cycling. Decomposition causes a 62% decrease in the elastic modulus of the Si anode, as measured by nanoindentation in electrolyte-soaked conditions. This study shows that an ultrathin polyamide coating counteracts this structural degradation, increases the elastic modulus of the degraded anode by 345%, and improves cohesion. Electrochemical analysis of polyamide-coated anodes reveals a film thickness dependence in cycling behavior. High overpotentials and fast capacity fading are observed for Si anodes with a 15 nm coating, whereas Si anodes with a 0.5 nm coating demonstrate stable cycling over 150 cycles with a capacity >1400 mAh g-1. Our findings identify polyamide as an effective electrode coating material to enhance structural integrity, leading to excellent cyclability with higher capacity retention. Furthermore, the use of the spatial MLD approach to deposit the coating enables short deposition time and a facile route to scale-up.

25 ENERGY STORAGE↗

Electrochemically induced fractures in crystalline silicon anodes

This communication presents our recent discovery on electrochemically induced fracture behavior of a single-crystal silicon (Si) anode, with particular focus on the initialization and propagation of cracks. Intensive efforts have investigated mechanical properties and cracking behavior of Si electrodes overextended electrochemical cycles. However, it is still elusive how cracks nucleate and propagate in the crystalline Si anodes at the very early stage. Here, we examined the morphology evolution of the Si (100) wafer electrodes during the first electrochemical cycle, and we found that the formation of <110>-oriented buckles - induced by the anisotropic lithiation in crystalline Si during 1st lithiation - results in cracks propagated along the <110> direction in the buckled region during 1st delithiation. Surprisingly, as the delithiation proceeds, new cracks oriented along the <100> direction appear in the intact area where no macroscopic deformation occurred during the previous lithiation. The <100>-oriented cracks have not been studied previously. Herein, we introduce a linear elastic fracture mechanics model to help understand underlying mechanisms for such crack propagation. The findings in this work provide significant insights into the fracture behavior and formation mechanism, as well as possible strategies to inhibit crack propagations of Si electrodes at the beginning stage of cycling.

25 ENERGY STORAGE↗

Three-dimensional electronic resistivity mapping of solid electrolyte interphase on Si anode materials

Silicon is a promising candidate for the lithium ion battery (LIB) anode because of the order-of-magnitude improvement in capacity over current state-of-the-art graphite anodes. In systems featuring both C and Si anodes, electronic resistivity of the solid-electrolyte interphase (SEI) layer is a critical factor for preventing continuous electrolyte-decomposition reactions at the electrode/electrolyte interface. However, the in-situ measurement of SEI electronic resistance has been complicated by ion transport and electronic contributions from other parts of the battery circuit. Ex-situ measurements of SEI resistivity at microscopic scales are also lacking. We report on a nanometer-resolution three-dimensional technique that enables ex-situ mapping of electronic resistivity of SEI formed on a model single-crystalline wafer Si anode. Our novel experimental approach uses scanning spreading-resistance microscopy resistance imaging and mechanical depth profiling. In addition to resistance mapping, this method also provides an alternative technique for locating buried interfaces, where mechanical or electronic properties differ sufficiently between layers. Further validation of this method was obtained by resistance mapping of a reference sample with a designed a-Si:H layer stack of different doping concentrations. The results show relatively uniform lateral resistivity distribution of the SEIs but steep decreases in resistivity in the vertical direction. Resistivity vs. depth profiles are highly dependent on cycling conditions, but they generally show a resistivity decrease from the most superficial levels of SEI and a thickness increase with continued cycling prior to SEI stabilization. The most prominent resistivity increase was observed on SEI formed in Gen2 electrolyte (EC:EMC [3:7 by wt.] + 1.2 M LiPF6) with 10 wt% fluoroethylene carbonate additive; this result may partially explain the significant improvements of sustained electrochemical cycling and coulombic efficiency observed with this electrolyte additive. Our approach provides a novel and unparalleled three-dimensional approach in characterizing electronic resistivity, which contributes significantly to understanding SEI formation and the intrinsic properties critical to battery performance.

25 ENERGY STORAGE↗

An artificial interphase enables reversible magnesium chemistry in carbonate electrolytes

Magnesium-based batteries possess potential advantages over their lithium counterparts. However, reversible Mg chemistry requires a thermodynamically stable electrolyte at low potential, which is usually achieved with corrosive components and at the expense of stability against oxidation. In lithium-ion batteries the conflict between the cathodic and anodic stabilities of the electrolytes is resolved by forming an anode interphase that shields the electrolyte from being reduced. This strategy cannot be applied to Mg batteries because divalent Mg 2+ cannot penetrate such interphases. Here, we engineer an artificial Mg 2+ -conductive interphase on the Mg anode surface, which successfully decouples the anodic and cathodic requirements for electrolytes and demonstrate highly reversible Mg chemistry in oxidation-resistant electrolytes. The artificial interphase enables the reversible cycling of a Mg/V 2 O 5 full-cell in the water-containing, carbonate-based electrolyte. This approach provides a new avenue not only for Mg but also for other multivalent-cation batteries facing the same problems, taking a step towards their use in energy-storage applications.

25 ENERGY STORAGE↗

Spatial atomic layer deposition for coating flexible porous Li-ion battery electrodes

Ultrathin atomic layer deposition (ALD) coatings on the electrodes of Li-ion batteries can enhance the capacity stability of the Li-ion batteries. To commercialize ALD for Li-ion battery production, spatial ALD is needed to decrease coating times and provide a coating process compatible with continuous roll-to-roll (R2R) processing. The porous electrodes of Li-ion batteries provide a special challenge because higher reactant exposures are needed for spatial ALD in porous substrates. This work utilized a modular rotating cylinder spatial ALD reactor operating at rotation speeds up to 200 revolutions/min (RPM) and substrate speeds up to 200 m/min. The conditions for spatial ALD were adjusted to coat flexible porous substrates. The reactor was initially used to characterize spatial Al2O3 and ZnO ALD on flat, flexible metalized polyethylene terephthalate foils. These studies showed that slower rotation speeds and spacers between the precursor module and the two adjacent pumping modules could significantly increase the reactant exposure. The modular rotating cylinder reactor was then used to coat flexible, model porous anodic aluminum oxide (AAO) membranes. The uniformity of the ZnO ALD coatings on the porous AAO membranes was dependent on the aspect ratio of the pores and the reactant exposures. Larger reactant exposures led to better uniformity in the pores with higher aspect ratios. The reactant exposures were increased by adding spacers between the precursor module and the two adjacent pumping modules. The modular rotating cylinder reactor was also employed for Al2O3 ALD on porous LiCoO2 (LCO) battery electrodes. Uniform Al coverages were obtained using spacers between the precursor module and the two adjacent pumping modules at rotation speeds of 25 and 50 RPM. The LCO electrodes had a thickness of ~49 um and pores with aspect ratios of ~12-25. Coin cells were then constructed using the ALD-coated LCO electrodes and were tested to determine their battery performance. The capacity of the Al2O3 ALD-coated LCO battery electrodes was measured versus the number of charge-discharge cycles. Both temporal and spatial ALD processing methods led to higher capacity stability compared with uncoated LCO battery electrodes. The results for improved battery performance were comparable for temporal and spatial ALD-coated electrodes. The next steps are also presented for scale-up to R2R spatial ALD using the modular rotating cylinder reactor.

25 ENERGY STORAGE↗