Effect of thermal spike on composite moisture capacity

As part of a continuing study of the effects of thermal spike on composite physical properties, severals sets of 16-ply TGDDM-DDS epoxy/graphite fiber composites were first saturated with moisture, and then individual specimens were subjected to thermal spikes of up to 240 C for periods of up to 25 minutes. At the cure temperature, 177 C, all sets show a change in rate of mass lost during spike. Post-spike moisture reabsorption capacity data provides evidence of temperature dependent molecular structural dilation and consolidation of the epoxide matrix. This evidence suggests that either a thermoreversible phenomenon such as physical aging or a nonreversible additional cure becomes active near the upper limit of the aircraft supersonic flight profile. These and other important observations suggest that one or more of several mechanisms may be active during thermal spike.

Adamson, M. J.

New experimental and analytical results for diffusion and swelling of resins used in graphite/epoxy composite materials

The epoxy resins currently in use can slowly absorb moisture from the atmosphere over a long period. This reduces those mechanical properties of composites which depend strongly on the matrix, such as compressive strength and buckling instabilities. The effect becomes greater at elevated temperatures. The paper will discuss new phenomena which occur under simultaneous temperature and moisture variations. An analytical model will also be discussed and documented.

Hiel, C. C.

New predictions methods for composites hygrothermal behavior

The methodology in this paper allows prediction of the thermal expansion and swelling of a composite material to temperature and moisture variations which typically occur in a launch environment. It is demonstrated that constitutive equations for moisture absorption and moisture-induced dimensional changes can be obtained with an internal variable method which is rooted in the theory of irreversible thermodynamics. Realism is injected into the model through the concept of free volume.

Hiel, C. C.

An internal variable assisted formulation of moisture sorption models for polymers and composites

The purpose of the paper is to demonstrate that constitutive equations for moisture sorption and swelling can be obtained with an internal variable method which is rooted in the theory of irreversible thermodynamics. Realism is injected into the model through the concept of free volume. The power of the method is illustrated by the solution of the formidable nonlinear boundary value problem for diffusion with swelling-stress dependent diffusivity.

Hiel, C. C.

A conceptual model of the thermal-spike mechanism in graphte/epoxy laminates

The influence of a thermal spike on a moisture-saturated graphite/epoxy composite was studied in detail. A single thermal spike from 25 to 132 C was found to produce damage, as evidenced by a significant increase in the level of moisture saturation in the composite. Approximately half of this increase remained after a vacuum-anneal at 150 C for seven days, suggesting the presence of an irreversible damage component. Subsequent thermal spikes created less and less additional moisture absorption, with the cumulative effect being a maximum or limiting moisture capacity of the composite. These observations are explained in terms of a model previously developed to explain the reverse thermal effect of moisture absorption in epoxy and epoxy-matrix composites. This model, based on the inverse temperature dependence of free volume, improves current understanding of thermal spike effects in graphite/epoxy composites.

Adamson, M. J.

A model of the thermal-spike mechanism in graphite/epoxy laminates

The influence of a thermal spike on a moisture-saturated graphite/epoxy composite was studied in detail. A single thermal spike from 25 C to 132 C was found to produce damage as evidenced by a significant increase in the level of moisture saturation in the composite. Approximately half of this increase remained after a vacuum anneal at 150 C for 7 days, suggesting the presence of an irreversible damage component. Subsequent thermal spikes created less and less additional moisture absorption, with the cumulative effect being a maximum or limiting moisture capacity of the composite. These observations are explained in terms of a model previously developed to explain the reverse thermal effect of moisture absorption in epoxy and epoxy matrix composites. This model, based on the inverse temperature dependence of free volume, contributes an improved understanding of thermal-spike effects in graphite/epoxy composites.

Adamson, M. J.

Failure of morphology of (0 deg)8 graphite/epoxy as influenced by environments and processing

Optical and scanning electron microscopy were used to investigate the failure morphology of graphite/epoxy specimens which had been tested until tensile failure. Failure morphology was studied as a function of the quality control variables of specimen preparation technique, prepreg batch, and cure condition, and also as a function of the environmental parameters of temperature and moisture content. Defective specimens were found to exhibit a low energy failure morphology. Poor specimen edge preparation and one batch of prepreg when tested at elevated temperature or moisture content also exhibited energy failure morphology. Postcuring had no effect on strength but did slightly alter failure morphology. Temperature or moisture appeared to decrease flaw sensitivity and thus increase strength; however, moisture also appeared to increase interfacial debonding between filament and matrix. When combined moisture and temperature increased interfacial debonding and made the epoxy matrix more prone to fracture.

Clements, L. L.

Thermal expansion and swelling of cured epoxy resin used in graphite/epoxy composite materials

The paper presents results of experiments in which the thermal expansion and swelling behavior of an epoxy resin system and two graphite/epoxy composite systems exposed to water were measured. It was found that the cured epoxy resin swells by an amount slightly less than the volume of the absorbed water and that the swelling efficiency of the water varies with the moisture content of the polymer. Additionally, the thermal expansion of cured epoxy resin that is saturated with water is observed to be more than twice that of dry resin. Results also indicate that cured resin that is saturated with 7.1% water at 95 C will rapidly increase in moisture content to 8.5% when placed in 1 C water. The mechanism for this phenomenon, termed reverse thermal effect, is described in terms of a slightly modified free-volume theory in conjunction with the theory of polar molecule interaction. Nearly identical behavior was observed in two graphite/epoxy composite systems, thus establishing that this behavior may be common to all cured epoxy resins.

Adamson, M. J.

Thermal Expansion and Swelling of Cured Epoxy Resin Used in Graphite/Epoxy Composite

The thermal expansion and swelling of resin material as influenced by variations in temperature during moisture absorption is discussed. Comparison measurements using composites constructed of graphite fibers and each of two epoxy resin matrices are included. Polymer theory relative to these findings is discussed and modifications are proposed.

Adamson, M. J.

Effects of moisture on torsion and flexure properties of graphite-epoxy composites

The effects of moisture and temperature on unidirectional and multi-ply laminates of T300/934 and AS/3501 graphite-epoxy systems were investigated. Properties studied were static flexure strength, and flexure and torsion fatigue strengths at room temperature and at 74 C. Specimens with increased moisture content showed a reduced static flexure strength; water as the test environment had only a negligible influence. In flexure fatigue and torsion fatigue, the water environment caused somewhat reduced fatigue strengths at room temperature and significantly greater degradation in 74 C water. The failure mode in all cases was interlaminar delamination.

Sumsion, H. T.

Effects of moisture on apparent flexure strength and on torsion and flexure fatigue properties of graphite-epoxy composites

The effects of moisture and temperature on unidirectional and multi-ply laminates of T300/934 and AS/3501 graphite-epoxy systems were investigated. Properties studied were static flexure strength and flexure and torsion fatigue strengths at room temperature and at 74 C. Specimens with increased moisture content showed a reduced static flexure strength; water as the test environment had only a negligible influence. In flexure fatigue and torsion fatigue, the water environment caused somewhat reduced fatigue strengths at room temperature and significantly greater degradation in 74 C water. The failure mode in all cases was interlaminar delamination.

Sumsion, H. T.

Stress-corrosion cracking due to hydrazine

Stress corrosion cracking susceptability in presence of hydrazine is examined for 6061-T6, Ti-6A1-4V(STA), Inconel 718, 410 stainless steel, and 4130 steel alloys.

Adamson, M. J.

Ultraviolet and thermally stable polymer compositions

A new class of polymers is provided, namely, poly (diarylsiloxy) arylazines. These novel polymers have a basic chemical composition which has the property of stabilizing the optical and physical properties of the polymer against the degradative effect of ultraviolet light and high temperatures. This stabilization occurs at wavelengths including those shorter than found on the surface of the earth and in the absence or presence of oxygen, making the polymers useful for high performance coating applications in extraterrestrial space as well as similar applications in terrestrial service. The invention also provides novel aromatic azines which are useful in the preparation of polymers such as those described.

Reinisch, R. F.

Electrical conductivity cell and method for fabricating the same

A flask having a threaded neck and a cap adapted for threaded engagement on the neck are used. A laminated disc between the cap and the neck forms a gas tight seal and the cap has a central opening that exposes a medial region of the disc. Piercing the disc through the opening are two electrodes, the inner ends of which contact the sample within the flask and the outer ends of which can be connected to test equipment. Cylindric glass tubes are fitted over the external portion of the electrodes to provide physical support and silicone rubber or a similar material serves to retain the glass cylinders in place and form a gas tight seal between the cylinders and the electrodes. Shrinkable tubing is shrunk over the glass tubes to afford further mechanical support and sealing. A final relatively large diameter shrinkable tube is shrunk over both electrodes and their associated glass cylinders. The support and sealing means for the electrodes is confined to a limited portion of the medial region of the disc so that the remainder of such region can be punctured by a hollow needle to introduce a test sample within the flask.

Gilbreath, W. P.

Aqueous stress-corrosion cracking of high-toughness D6AC steel

The crack growth behavior of D6AC steel as a function of stress intensity, stress and corrosion history, and test technique, under sustained load in filtered natural seawater, 3.3 per cent sodium chloride solution, and distilled water, was investigated. Reported investigations of D6AC were considered in terms of the present study with emphasis on thermal treatment, specimen configuration, fracture toughness, crack-growth rates, initiation period, and threshold. Both threshold and growth kinetics were found to be relatively insensitive to these test parameters. The apparent incubation period was dependent on technique, both detection sensitivity and precracking stress intensity level.

Gilbreath, W. P.

The effect of heat treatment and test parameters on the aqueous stress corrosion cracking of D6AC steel

The crack growth behavior of D6AC steel as a function of stress intensity, stress and corrosion history and test technique, under sustained load in natural seawater, 3.3 percent NaCl solution, distilled water, and high humidity air was investigated. Reported investigations of D6AC were considered with emphasis on thermal treatment, specimen configuration, fracture toughness, crack-growth rates, initiation period, threshold, and the extension of corrosion fatigue data to sustained load conditions. Stress history effects were found to be most important in that they controlled incubation period, initial crack growth rates, and apparent threshold.

Gilbreath, W. P.

Ultraviolet and thermally stable polymer compositions

A class of polymers is provided, namely, poly(diarylsiloxy) arylazines. These polymers have a basic chemical composition which has the property of stabilizing the optical and physical properties of the polymer against the degradative effect of ultraviolet light and high temperatures. This stabilization occurs at wavelengths including those shorter than found on the surface of the earth and in the absence or presence of oxygen, making the polymers of the present invention useful for high performance coating applications in extraterrestrial space as well as similar applications in terrestrial service. The invention also provides aromatic azines which are useful in the preparation of polymers such as those of the present invention.

Reinisch, R. F.

Poly/diphenylsiloxy/arylazines. I - Synthesis and characterization

A detailed description is presented for the synthesis of poly(diphenylsiloxy)arylazines by the melt polymerization of hydroxyarylazines and bis(anilino)diphenylsilane. The resulting polymers have been characterized by elemental analysis, gel-permeation chromatography, vapor-phase osmometry, and UV-VIS-IR optical spectroscopy.

Goldsberry, R. E.